Polymer Property : Thickness = 2.53 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 64.3 microns
2.53 mil
estimated wet film thickness
Aremco Corr-Paint™ CP4050 High Temperature Protective Coating Silicone
Low viscosity, green coating for power resistors to 1100°F (593°C)