Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4000 High Temperature Protective Silicone Coating, Metal Oxide Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4010S High Temperature Protective Coating Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4020-S High Temperature Protective Coating Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4040-S High Temperature Protective Coating Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4050 High Temperature Protective Coating Silicone Low viscosity, green coating for power resistors to 1100°F (593°C) |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4060 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4060-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4070-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4095-S High Temperature Protective Coating, Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco HiE-Coat™ 840-MS High Emissivity Coating, Silicone-Ceramic Filled Silicone-ceramic, black pigmented single component coating for aluminum, brass, copper, and carbon and stainless steel to 1100 °F (593 °C). |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Lamp-Coat™ LC4010-GL High Temperature Coating, Silicone Aluminum-filled coating for application directly over uncoated headlamps to 1020 ºF (550 ºC) |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Aremco-Seal™ 4030 High Temperature Specialty Coatings Silicone, Ceramic Filled Translucent-white, low-viscosity sealer for porous materials to 900°F (482°C) |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4000-S High Temperature Protective Coating Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4010 High Temperature Protective Silicone Coating, Aluminum Filled Single part, silicone-based, low viscosity, heat-curable, aluminum-filled sealer offering exceptional moisture resistance to 1100°F (593°C). |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4020 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4010 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4070 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4090-S High Temperature Protective Coating, Silicone-Polyester |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4095 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Glass-Coat™ SGC4000 High Temperature Specialty Coatings Silicone-Glass Silicone-glass-ceramic, gray, low viscosity, scratch resistant coating for stainless steel to 900°F (482°C) |
|||
Processing Temperature | 10.0 - 48.9 °C | 50.0 - 120 °F | Application Temperature |
Aremco Lamp-Coat™ LC4040-SG High Temperature Coating, Silicone White reflective coating for use on mercury vapor lamps and other high temperature glass and quartz components to 1200 ºF (649 ºC). |