Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 500 - 600 cP | 500 - 600 cP | |
ND Industries 360 Surface Insensitive Instant Superglue General DescriptionA medium viscosity, general purpose cyanoacrylate which is also surface sensitive. Can handle a wide array of materials which include wood, cork, leather, stone and plastics, in .. |
|||
Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
Uncured |
Permabond HM128 Anaerobic Threadlocker Permabond® HM128 Threadlocker is a high strength adhesive for permanent assembly. It is typically used for preventing vibration loosening of bolts, studs and cap screws. Full cure to a cross-linked.. |
|||
Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
Uncured |
Permabond HM129 Anaerobic Threadlocker Permabond® HM129 is a high strength medium viscosity anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. Cure is fast and reliable on st.. |
|||
Viscosity | 500 cP | 500 cP | |
Resinlab® CYNERGY CA6703 Adhesive Description: The CYNERGY 6700 SERIES are modified to provide greatly reduced odor and a further reduction of bloom or frosting of plastics when compared to the 6600 Series. These products are ideal .. |
|||
Viscosity | 500 cP | 500 cP | |
Resinlab® RC8048 Anaerobic Retaining Compound The RC 8000 Series anaerobic retaining compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. These products .. |
|||
Viscosity | 500 cP | 500 cP | Nominal |
Resin Technology Group UV CC-2004 Multi-Functional, UV Curing, Conformal-Coating Multi-functional UV-CC 2004 is a single component, solvent-less conformal-coating specifically formulated for rapid room temperature cure when exposed to UV light. Thin layer coatings cure almost in.. |
|||
Viscosity | 500 cP | 500 cP | |
Resinlab® CYNERGY CA6807 Adhesive Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP .. |
|||
Viscosity | 500 - 900 cP | 500 - 900 cP | |
Huntsman HY 955 Polyamide Approx. H+ equivalent weight 65. Mix Ratio with GY 6010 is 35.Comments/Applications: Modified liquid amidoamine, low viscosity. Adhesives, coatings, flooring, potting and we lay-up applications. .. |
|||
Viscosity | 500 - 900 cP | 500 - 900 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-422 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo.. |
|||
Viscosity | 500 - 1200 cP | 500 - 1200 cP | #2 SP. @30 RPM; RP-0659 |
Solvay ALKASPERSE® A-5H Surfactant Chemical Name: PARTIAL SODIUM SALT OF POLYACRYLIC ACIDCAS: 9003-01-4, 9003-04-7 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKASPERSE© A-5H is a solid disper.. |
|||
Viscosity | <= 500 cP | <= 500 cP | #3 SP. @12 rpm |
Solvay MACKAM® 2CSF-40CG Surfactant Product Description: Mackam 2CSF-40CG is an alcohol and salt free, mild, amphoteric surfactant with applications in both personal care and industrial formulations. In personal care products, Mackam .. |
|||
Viscosity | <= 500 cP | <= 500 cP | #3 SP @ 12 rpm |
Solvay MACKAM® HPC 32L Surfactant Product Description: Mackam HPC-32L is a high purity amphoteric, preservative free, surfactant that is suggested as a mild component for personal care or industrial products. Mackam HPC-32L has a hi.. |
|||
Viscosity | 500 - 2000 cP | 500 - 2000 cP | #2 SP. @30 RPM; RP-0596 |
Solvay ALKAMIDE® AK50BN Surfactant Chemical Name: TALL OIL DIETHANOLAMIDEINCI NAME: Tallowamide DEACAS: 68155-20-4; 111-42-2; 67-56-1; 61790-12-3Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKAMID.. |
|||
Viscosity | 500 - 2500 cP | 500 - 2500 cP | Milled Cement; Zeon Test #327 |
Zeon Chemicals Nipol® 1031 Nitrile Elastomer Nipol 1031 is a copolymer of butadiene and acrylonitrile with very high oil resistance. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Excellent fuel a.. |
|||
Viscosity | 500 cP | 500 cP | Dynamic |
Dow Corning SYL-OFF® PMCP7137 High Speed Crosslinker Syl-Off® 7137 High Speed Crosslinker is a 100% active solids crosslinker additive. Recommended for high speed coating conditions where generation of silicone mist is an issue.Information provided b.. |
|||
Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
|
Cytec (Conap) RN-1000 / EA-028 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
|
Esstech X-829-7100 PMGDM, 50% (w/w) Solution in Triethyleneglycol Dimethacrylate, C32H34O16 Dissolving pyromellitic glycerol dimethacrylate or PMGDM in triethyleneglycol dimethacrylate rather than acetone decreases the polarity and odor of this system. The low volatility of TEGDMA also ext.. |
|||
Viscosity | 500 cP | 500 cP | dynamic |
Dow Corning 3-4170 DIELECTRIC GEL KIT Two-part, clear, heat cure, long working time.Information provided by Dow Corning |
|||
Viscosity | 500 cP | 500 cP | |
Dymax 3092 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Viscosity | 500 - 2500 cP @Temperature 25.0 °C |
500 - 2500 cP @Temperature 77.0 °F |
spindle n 3-10 RPM; MA143LFE |
C.O.I.M. FILCO® 650 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Aremco Corr-Paint™ CP4080 High Temperature Protective Coating Silicone, Aluminum Filled This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a.. |
|||
Viscosity | 500 cP | 500 cP | |
Aremco Crystalbond™ 555-HMP Washaway Mounting Adhesive & Accessory Low melting point adhesive systems for moderate-stress machining processes, dry plasma etching of silicon wafers and de-paneling copper plated Teflon boards. Transparent in thin cross-sections. Solu.. |
|||
Viscosity | 500 - 1000 cP | 500 - 1000 cP | |
Aremco Ceramacoat™ 845-BLU High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, blue coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu.. |
|||
Viscosity | 500 cP | 500 cP | |
Aremco Crystalbond™ 555 Washaway Mounting Adhesive & Accessory Low melting point adhesive systems for moderate-stress machining processes, dry plasma etching of silicon wafers and de-paneling copper plated Teflon boards. Transparent in thin cross-sections. Solu.. |
|||
Viscosity | 500 - 1500 cP | 500 - 1500 cP | |
Aremco Pyro-Paint™ 634-BN High Temperature Refractory Coating This highly-filled boron nitrite solution is extremely lubricious and inert. They are non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN f.. |
|||
Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
Uncured |
Permabond A011 Anaerobic Threadlocker Permabond® A011 is an anaerobic adhesive designed for locking and sealing threaded or coaxially fitting metal parts where subsequent dismantling is required. Its controlled strength ensures fatigue.. |
|||
Viscosity | 500 cP | 500 cP | QSil 216B |
ACC QSil 216 QSI Quantum Silicones Transparent Liquid Silicone Rubber QSil 216 is a two-part, clear, liquid silicone which will cure at room temperature or at elevated temperatures. It has a low viscosity, which allows for ease of flow around complex parts, providing .. |
|||
Viscosity | 500 cP | 500 cP | |
Loctite® 661 Retaining Compound RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. .. |