Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 500 - 700 cP | 500 - 700 cP | |
ND Industries SuperGlue Ethyl 344 Medium viscosity, general purposeMeets military spec Mil-A-46050C Type II Class III |
|||
Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
Uncured |
Permabond HM128 Anaerobic Threadlocker Permabond® HM128 Threadlocker is a high strength adhesive for permanent assembly. It is typically used for preventing vibration loosening of bolts, studs and cap screws. Full cure to a cross-linked.. |
|||
Viscosity | 500 cP | 500 cP | |
Resinlab® CYNERGY CA6007 Adhesive Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety.. |
|||
Viscosity | 500 cP | 500 cP | Nominal |
Resin Technology Group UV CC-2004 Multi-Functional, UV Curing, Conformal-Coating Multi-functional UV-CC 2004 is a single component, solvent-less conformal-coating specifically formulated for rapid room temperature cure when exposed to UV light. Thin layer coatings cure almost in.. |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Huntsman Araldite GY 507 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 180 to 192. Max color is 3.Comments/Applications: GY 6010 modified with DY 023 (CGE) - a monofunctional reactive diluent. General purpose, modified resin. Very low .. |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Huntsman Araldite GY 509 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 189 to 200. Max color is 1.Comments/Applications: GY 6010 cut with DY 027 (Epoxide 7). Longer pot life, lower exotherm. General purpose low viscosity resin.Data pro.. |
|||
Viscosity | 500 - 900 cP | 500 - 900 cP | |
Huntsman HY 955 Polyamide Approx. H+ equivalent weight 65. Mix Ratio with GY 6010 is 35.Comments/Applications: Modified liquid amidoamine, low viscosity. Adhesives, coatings, flooring, potting and we lay-up applications. .. |
|||
Viscosity | 500 - 850 cP | 500 - 850 cP | 15% Toluene Solution at 25°C; BAM 922 |
Kraton® G1641 H (SEBS) Linear Triblock Copolymer Description: Kraton G1641 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 33%. It is supplied from North America in the physical form ide.. |
|||
Viscosity | 500 - 900 cP | 500 - 900 cP | 15% solids in MEK |
Taiwan Sheen Soon Sheenthane® AS-422 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo.. |
|||
Viscosity | 500 cP | 500 cP | |
Silikony Polskie Polastosil M-500 Silicone Rubber Diluent |
|||
Viscosity | 500 - 1200 cP | 500 - 1200 cP | #2 SP. @30 RPM; RP-0659 |
Solvay ALKASPERSE® A-5H Surfactant Chemical Name: PARTIAL SODIUM SALT OF POLYACRYLIC ACIDCAS: 9003-01-4, 9003-04-7 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: ALKASPERSE© A-5H is a solid disper.. |
|||
Viscosity | <= 500 cP | <= 500 cP | RP-17619 |
Solvay RHODACAL® A-246/L Surfactant Description: X High-foaming detergent and emulsifier. Alkali stable. Also used as a foam booster, dispersant and wetter in dishwashing, car- wash products and general- purpose cleaners.Chemical Name.. |
|||
Viscosity | 500 cP @Temperature 25.0 °C |
500 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Cast 3010 Flexible Clear Epoxy Casting Compound TRA-CAST 3010 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties, good clarity, long pot life.. |
|||
Viscosity | 500 - 1000 cP @Temperature 23.0 °C |
500 - 1000 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy Product Description: EPO-TEK® 377H is a two component, high Tg, graphite filled epoxy designed for ESD/EMI shielding of semiconductor devices and electronics. It can be used in many electronic ind.. |
|||
Viscosity | 500 cP | 500 cP | |
Dymax 3092 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Viscosity | 500 cP | 500 cP | |
Abatron AboCast 8503-4/AboCure 8503-4 Colorless Epoxy AboCast 8503-4/AboCure 8503-4 is a general purpose, moderate speed, colorless epoxy casting compound with low viscosity. It offers a convenient 2/1 ratio by volume and lends itself to casting of thi.. |
|||
Viscosity | 500 - 3000 cP @Temperature 25.0 °C |
500 - 3000 cP @Temperature 77.0 °F |
spindle n 3-10 RPM; MA143LFE |
C.O.I.M. FILCO® 362 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Viscosity | 500 - 2500 cP @Temperature 25.0 °C |
500 - 2500 cP @Temperature 77.0 °F |
spindle n 3-10 RPM; MA143LFE |
C.O.I.M. FILCO® 650 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Aremco Corr-Paint™ CP4060-S High Temperature Protective Coating, Silicone-Polyester |
|||
Viscosity | <= 500 cP | <= 500 cP | Bulk |
3M Polystyrene Foam Insulation 78 Spray Adhesive A high strength, industrial grade spray adhesive that is typically used for bonding most types of insulation such as fiberglass, expanded polystyrene foam, and extruded polystyrene foam.Features:Agg.. |
|||
Viscosity | <= 500 cP | <= 500 cP | |
3M Scotch-Weld™ Hi-Strength Postforming 94 CA Spray Adhesive A low VOC, high performance, postformable grade spray adhesive with a unique low telegraphing pebble spray pattern.Features:Bonds to a variety of demanding substrates like decorative laminate, metal.. |
|||
Viscosity | 500 - 1000 cP | 500 - 1000 cP | |
Aremco Ceramacoat™ 845-BLU High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, blue coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu.. |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Aremco Corr-Paint™ CP4095-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 500 - 1500 cP | 500 - 1500 cP | |
Aremco Pyro-Paint™ 634-BN High Temperature Refractory Coating This highly-filled boron nitrite solution is extremely lubricious and inert. They are non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN f.. |
|||
Viscosity | 500 cP | 500 cP | |
Loctite® 661 Retaining Compound RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. .. |
|||
Viscosity | 500 cP | 500 cP | |
Loctite® 648 High Strength/Rapid Cure Retaining Compound RetainersLoctite Corporation, the pioneer of anaerobic adhesives, has applied this technology to create retaining compounds that increase the shear strength of cylindrical, non-threaded assemblies. .. |
|||
Viscosity | 500 - 700 cP | 500 - 700 cP | |
Huntsman Araldite GY 9667 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 196 to 212. Max color is 2.Comments/Applications: GY 6020 modified with DY 025 (Epoxide 8) for less crystallization and improved elongation. High solids and solvent .. |