Material Notes:
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxidation, ozone and general outdoor weathering is excellent.Processing: compatible with polypropylene for co-molding or co-extrusion Can be used in food contact applications with the appropriate stabilizer package
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ISO 2782
Viscosity Measurement 9.0

@Temperature 180 °C
9.0

@Temperature 356 °F
Kg/cm<sup>2</sup>; Macklow-Smith extrusion rheometer
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
ISO 868
Tensile Strength 13.4 MPa
1940 psi
ISO 37
Elongation at Break 560 %
560 %
ISO 37
100% Modulus 0.00300 GPa
0.435 ksi
ISO 37
Tear Strength 45.0 kN/m
257 pli
ISO 34-B
Compression Set 41 %

@Temperature 22.0 °C,
Time 259000 sec
41 %

@Temperature 71.6 °F,
Time 72.0 hour
ISO 815
49 %

@Temperature 70.0 °C,
Time 79200 sec
49 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
70 %

@Temperature 100 °C,
Time 79200 sec
70 %

@Temperature 212 °F,
Time 22.0 hour
ISO 815
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 - 120 °C
230 - 248 °F
Minimum Service Temperature, Air -60.0 - -40.0 °C
-76.0 - -40.0 °F
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Dielectric Strength 24.0 - 28.0 kV/mm
610 - 711 kV/in
Descriptive Properties Value Comments
Bonds with Polypropylene
Chemical Resistance Acetone
Moderate/Good
Acids up to 80%
Excellent
Alcohol
Excellent
Alkalis
Excellent
Brake fluid
Good
Chlorinate solvents
Poor
Diesel
Poor
Ethylene glycol
Excellent
Gasoline
Poor
Salt solution
Excellent
Soda lye
Excellent
Water, 23°C
Excellent
Water, 95°C
Good
Transparency Opaque