Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 17.3 - 28.0 kV/mm | 439 - 711 kV/in | Average value: 24.9 kV/mm Grade Count:7 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Dielectric Strength | 24.0 - 28.0 kV/mm | 610 - 711 kV/in | |
AlphaGary Evoprene™ G 3290 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Dielectric Strength | 24.0 - 28.0 kV/mm | 610 - 711 kV/in | |
AlphaGary Evoprene™ G 927 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Dielectric Strength | 24.0 - 28.0 kV/mm | 610 - 711 kV/in | |
AlphaGary Evoprene™ G 958 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Dielectric Strength | 24.0 - 28.0 kV/mm | 610 - 711 kV/in | |
AlphaGary Evoprene™ G 964 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Dielectric Strength | 24.0 - 28.0 kV/mm | 610 - 711 kV/in | |
AlphaGary Evoprene™ G 966 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Dielectric Strength | 24.0 - 28.0 kV/mm | 610 - 711 kV/in | |
AlphaGary Evoprene™ G 975 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Dielectric Strength | 24.0 - 28.0 kV/mm | 610 - 711 kV/in | |
AlphaGary Evoprene™ G 991 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Dielectric Strength | 24.0 - 28.0 kV/mm | 610 - 711 kV/in | |
AlphaGary Evoprene™ G 992 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |