Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -55.0 - -40.0 °C | -67.0 - -40.0 °F | Average value: -51.7 °C Grade Count:39 |
Overview of materials for Methacrylate Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Methacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Minimum Service Temperature, Air | -55.0 - -40.0 °C | -67.0 - -40.0 °F | Average value: -46.7 °C Grade Count:3 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Minimum Service Temperature, Air | -115 - -40.0 °C | -175 - -40.0 °F | Average value: -68.5 °C Grade Count:32 |
Overview of materials for Silicone, RTV, Encapsulation Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Encapsulation Grade". Each property range of values reported is minimum and maximum value.. |
|||
Minimum Service Temperature, Air | -136 - -40.0 °C | -212 - -40.0 °F | Average value: -58.5 °C Grade Count:491 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Minimum Service Temperature, Air | -136 - -40.0 °C | -212 - -40.0 °F | Average value: -58.4 °C Grade Count:672 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Minimum Service Temperature, Air | -100 - -40.0 °C | -148 - -40.0 °F | Average value: -55.0 °C Grade Count:3 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Minimum Service Temperature, Air | -60.0 - -40.0 °C | -76.0 - -40.0 °F | |
AlphaGary Evoprene™ G 3290 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Minimum Service Temperature, Air | -60.0 - -40.0 °C | -76.0 - -40.0 °F | |
AlphaGary Evoprene™ G 927 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Minimum Service Temperature, Air | -60.0 - -40.0 °C | -76.0 - -40.0 °F | |
AlphaGary Evoprene™ G 958 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Minimum Service Temperature, Air | -60.0 - -40.0 °C | -76.0 - -40.0 °F | |
AlphaGary Evoprene™ G 964 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Minimum Service Temperature, Air | -60.0 - -40.0 °C | -76.0 - -40.0 °F | |
AlphaGary Evoprene™ G 966 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Minimum Service Temperature, Air | -60.0 - -40.0 °C | -76.0 - -40.0 °F | |
AlphaGary Evoprene™ G 975 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Minimum Service Temperature, Air | -60.0 - -40.0 °C | -76.0 - -40.0 °F | |
AlphaGary Evoprene™ G 991 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Minimum Service Temperature, Air | -60.0 - -40.0 °C | -76.0 - -40.0 °F | |
AlphaGary Evoprene™ G 992 SEBS Thermoplastic Elastomer Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi.. |
|||
Minimum Service Temperature, Air | -100 - -40.0 °C | -148 - -40.0 °F | Average value: -52.9 °C Grade Count:11 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |