Material Notes:
Information provided by Sylvin Technologies Inc.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
10 seconds
Tensile Strength, Ultimate 10.3 MPa
1500 psi
Elongation at Break 500 %
500 %
Tear Strength Test 200
200
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 154 - 166 °C
310 - 330 °F