Addiplast Addilene PMD 50265 Flame Retardant Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer Addiplast
Trade Name Addilene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addiplast Addilene PMD 50265 Flame Retardant Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame retardant, high rigidityInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ISO 1183/A
Melt Flow 16 g/10 min
16 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
Conditioned; ISO 868
Tensile Strength at Break 30.0 MPa
4350 psi
Conditioned; ISO R 527
Elongation at Break 5.0 %
5.0 %
Conditioned; ISO R 527
Modulus of Elasticity 2.00 GPa
290 ksi
Conditioned; ISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
Conditioned; ISO 180/1A
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.700 J/cm²
3.33 ft-lb/in²
Conditioned; ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 165 - 168 °C
329 - 334 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ISO 75-2/AF
Vicat Softening Point 150 °C
302 °F
ISO 306/A50
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Oxygen Index 17 %
17 %
ISO 4589
Glow Wire Test 750 °C
1380 °F
CEI 60695/2/1
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
Conditioned; CEI 60093
Surface Resistance >= 1.00e+13 ohm
>= 1.00e+13 ohm
Conditioned; CEI 60093
Comparative Tracking Index >= 600 V
>= 600 V
CEI 60112/Solution A
Users viewing this material also viewed the following: