Material Notes:
QSil 550 is a 100% silicone solids elastomer designed for electrical potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairable. Key Features: 100% solids Long gel time Good elongation Low modulusPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
"B" component
1.41 g/cc
1.41 g/cc
"A" component
Viscosity 4000 cP
4000 cP
"B" component
4000 cP
4000 cP
"A" component
Storage Temperature <= 38.0 °C
<= 100 °F
12 months
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
cured 7 mins @ 150°C
Tensile Strength, Yield 3.52 MPa
511 psi
cured 7 mins @ 150°C
Elongation at Break 150 %
150 %
cured 7 mins @ 150°C
Tear Strength 5.78 kN/m
33.0 pli
cured 7 mins @ 150°C
Thermal Properties Metric English Comments
Thermal Conductivity 0.370 W/m-K
2.57 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C
399 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.47e+15 ohm-cm
1.47e+15 ohm-cm
Dielectric Constant 3.1

@Frequency 1000 Hz
3.1

@Frequency 1000 Hz
Dissipation Factor 0.0030
0.0030
Processing Properties Metric English Comments
Gel Time 130 min
130 min
Descriptive Properties Value Comments
Color Beige
"A" component
Black
"B" component
Users viewing this material also viewed the following: