Physical Properties | Metric | English | Comments |
---|---|---|---|
Storage Temperature | 38.0 °C | 100 °F | 6 months time; FTM 3467 |
ExxonMobil Mobilgrease 28 Mobilgrease 28 is a supreme performance, wide-temperature, antiwear grease designed to combine the unique features of a polyalphaolefin (PAO) synthetic base fluid with an organo-clay (non-soap) thic.. |
|||
Storage Temperature | 38.0 °C | 100 °F | 6 months time; FTM 3467 |
ExxonMobil Mobilgrease 28 Mobilgrease 28 is a supreme performance, wide-temperature, antiwear grease designed to combine the unique features of a polyalphaolefin (PAO) synthetic base fluid with an organo-clay (non-soap) thic.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QGel 300 QSI Quantum Silicones High Strength Gel QGel 300 is a clear, very soft, tough, moderately cross-linked, silicone polymer. Silicone gels are used to provide protection from vibration, thermal or mechanical shock. Silicone gels also provide.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QGel 301 QSI Quantum Silicones High Strength Gel QGel 301 is a clear, very soft, tough, moderately cross-linked, silicone polymer. Silicone gels are used to provide protection from vibration, thermal or mechanical shock. Silicone gels also provide.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QGel 311 QSI Quantum Silicones General Purpose Silicone Gel QGel 311 is a clear, fast cure, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QGel 315 QSI Quantum Silicones General Purpose Silicone Gel QGel 315 is a clear, very soft, tough moderately cross-linked silicone polymer. Silicone gels are used to provide protection from vibration and thermal or mechanical shock. Silicone gels also provid.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QLE 1020 QSI Quantum Silicones 45 Durometer Clear, Addition Cure Elastomer for Coating QLE 1020 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QLE 1031 QSI Quantum Silicones 25 Durometer Addition Cure Elastomer for Coating QLE 1031 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QLE 1039 QSI Quantum Silicones 40 Durometer Addition Cure Elastomer for Coating QLE 1039 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QLE 1101 QSI Quantum Silicones Specialty Silicone Coating QLE 1101 is a low viscosity, two-component, addition cure, silicone elastomer.Key Features: Fast cure at elevated temperaturesLow linear shrinkageTransparent, ideal for pigmentationLow viscosity Par.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 6 months |
ACC QM 100 QSI Quantum Silicones Clear 30 Durometer Condensation Cure Material QM 100 is a two component, room temperature condensation cure silicone material. The cured rubber is a crystal clear material designed specifically for the special effects market. The materials' cla.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 6 months |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 6 months |
ACC QM 122 QSI Quantum Silicones 22 Durometer Condensation Cured Moldmaking Material QM 122 is a two-component, room temperature condensation cure silicone material. The cured rubber is flexible with excellent mechanical and physical properties in addition to good shelf-life stabili.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 6 months |
ACC QM 135 QSI Quantum Silicones 35 Durometer Condensation Cured Moldmaking Material QM 135 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 6 months |
ACC QM 140 QSI Quantum Silicones 40 Durometer Condensation Cured Moldmaking Material QM 140 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QM 230 QSI Quantum Silicones 30 Durometer Addition Cure Moldmaking Material QM 230 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QM 230F QSI Quantum Silicones 30 Durometer Addition Cure Moldmaking Material QM 230F is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for t.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QM 245 QSI Quantum Silicones 45 Durometer Addition Cure Moldmaking Material QM 245 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QM 260 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM 260 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for th.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QM 264 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM 264 is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin .. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 6 months |
ACC QM Skin 30 QSI Quantum Silicones 30 Durometer Condensation Cure moldmaking Material QM Skin 30 is a two-component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and very low bleed in addition to good shelf-l.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 6 months |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 6 months |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QSil 550 QSI Quantum Silicones Silicone Potting Material QSil 550 is a 100% silicone solids elastomer designed for electrical potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairab.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QSil 550R QSI Quantum Silicones Silicone Potting Material QSil 550Ris a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairab.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QSil 550SB QSI Quantum Silicones Self-Priming Silicone Potting Material QSil 550SB is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repair.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QM 262F QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM 262F is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 12 months |
ACC QSil 553 QSI Quantum Silicones Silicone Potting Material QSil 553 is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a flame retardant, thermally conductive, low modulus material that is readi.. |
|||
Storage Temperature | <= 38.0 °C | <= 100 °F | 6 months |
ACC QSil 12 QSI Quantum Silicones Clear Low Viscosity for Potting Material QSil 12 is a clear, transparent, low viscosity, two-component, liquid silicone material which cures at room temperature and is primarily intended for potting applications. This material is typically.. |
|||
Storage Temperature | 38.0 °C | 100 °F | 6 months time; FTM 3467 |
ExxonMobil Mobilgrease 27 Mobilgrease 27 is a high performance, aviation grease designed to combine the unique features of a synthetic ester base fluid with a lithium soap thickener. Its consistency is between an NLGI No. 1 .. |