Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.52 MPa
511 psi
at 200%, as molded
Multibase SILASTIC® C7-4565 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Yield 3.52 MPa
510 psi
at 200%, post cured- 2 hours at 177°C
Multibase SILASTIC® C7-4565 VAROX Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tensile Strength, Yield 3.52 MPa
510 psi
at 100%; ASTM D412
2074A Polyurethane-based Biomedical Elastomer
Tensile Strength, Yield 3.52 MPa
510 psi
200%, post cured- 8 hours at 177°C; ASTM D412
Multibase C6-265 PERKADOX PD-50S Dow-Corning Class VI Elastomer
Information provided by Multibase
Tensile Strength, Yield 3.52 MPa
511 psi
ASTM D412
Teknor Apex Uniprene® UN-7010-45NT Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin..
Tensile Strength, Yield 3.52 MPa
511 psi
cured 7 mins @ 150°C
ACC QSil 550 QSI Quantum Silicones Silicone Potting Material
QSil 550 is a 100% silicone solids elastomer designed for electrical potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairab..
Tensile Strength, Yield 3.52 MPa
510 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-3630 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:Consumer GoodsIndustrialProcessing Method:Injection MoldingPolyOne First ChoiceInformation..
Tensile Strength, Yield 3.52 MPa

@Strain 100 %
511 psi

@Strain 100 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ HTE 1106 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)