Polymer Property : Tear Strength = 5.78 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 5.78 kN/m
33.0 pli
cured 7 mins @ 150°C
ACC QSil 550 QSI Quantum Silicones Silicone Potting Material
QSil 550 is a 100% silicone solids elastomer designed for electrical potting applications. The two-component system offers a hard, thermally conductive, low modulus material that is readily repairab..
Tear Strength 5.78 kN/m
33.0 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® RT-3605 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Multi-Purpose Thermoplastic ElastomerNaturalApplications:General PurposeInteriorMarket:IndustrialConsumer GoodsProcessing Method:Injection MoldingInformation provided by PolyOne..