Material Notes:
QM 230F is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for the molding of furniture, picture frames and architectural materials. QM 230F is exceptionally good where highly detailed parts and mold flexibility are required. QM 230F has a shorter work life than QM 230 and QM 230 Clear. Material complies with FDA indirect food contact regulation CFR 177.2600Key Features: Low viscosity Fast demold time Casting resin resistance Excellent flexibilityMain Applications: Molds for architectural replication Molds for polyester, polyurethane and epoxy resin castings Molds for technical articles and prototype Molds for furniture and picture frame replication Candy and other food moldsPart of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
Uncatalyzed, QM 230F B
1.32 g/cc
1.32 g/cc
Base
Viscosity 200 cP
200 cP
Uncatalyzed, QM 230F B
10000 cP
10000 cP
catalyzed with QM 230F B
17000 cP
17000 cP
Base
Linear Mold Shrinkage <= 0.0010 cm/cm
<= 0.0010 in/in
cured 72 hrs @ RT
Storage Temperature <= 38.0 °C
<= 100 °F
12 months
Mechanical Properties Metric English Comments
Hardness, Shore A 33
33
cured 72 hrs @ RT
Tensile Strength, Yield 2.90 MPa
421 psi
cured 72 hrs @ RT
Elongation at Break 500 %
500 %
cured 72 hrs @ RT
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
399 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Processing Properties Metric English Comments
Dry Time 4 - 6 hour
4 - 6 hour
Demold time, catalyzed with QM 230F B
Descriptive Properties Value Comments
Color Beige
Base
Blue
catalyzed with QM 230F B
Dark Blue
Uncatalyzed, QM 230F B
Work Life 12 min
catalyzed with QM 230F B