Axiall 21570 Coax & Telecom Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 21570 Coax & Telecom Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Semi-rigid insulation compound designed for data communication riser cable applications. Maximum 75°C service temperature rating.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.31 - 1.35 g/cc
1.31 - 1.35 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 54 - 60
54 - 60
delayed; ASTM D-2240
Tensile Strength, Yield 22.8 MPa
3300 psi
ASTM D-638
Elongation at Yield 275 %
275 %
ASTM D-638
100% Modulus 0.0190 GPa
2.75 ksi
ASTM D-638
Thermal Properties Metric English Comments
Brittleness Temperature -15.0 °C
5.00 °F
ASTM D-746
Oxygen Index 33 %
33 %
ASTM D-638
Electrical Properties Metric English Comments
Dielectric Constant 3.65

@Frequency 1000 Hz
3.65

@Frequency 1000 Hz
Processing Properties Metric English Comments
Melt Temperature 196 °C
385 °F