Polymer Property : Specific Gravity = 0.970 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM 792
Multibase Nylex™ 2185 NAT Polyamide + PP
Features: Crack Resistance, GoodDimensional Stability, GoodImpact Resistance, GoodMoisture ResistantProcessability, GoodForms:PelletsProcessing Methods:Injection MoldingUses: Electrical PartsHousing..
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM 792
Multibase Nylex™ 2185 Polyamide + PP
Forms: PelletsInformation provided by Multibase
Specific Gravity 0.970 - 0.990 g/cc
0.970 - 0.990 g/cc
Michelman® Michem® Lube 723 Nonionic paraffin wax emulsion
Description: Nonionic paraffin wax emulsionUsage: Michem® Lube 723 provides excellent water repellancy, lubricity, release and wood end check protection when used in the paint and coatings indust..
Specific Gravity 0.970 - 0.990 g/cc
0.970 - 0.990 g/cc
Michelman® Michem® Tite 242AF Skin packaging primer
Description: Skin packaging primerUsage: Michem® Tite 242AF is a coating designed to provide a tenacious bond between corrugated and either Surlyn or polyethylene clear skin pack films, firmly tr..
Specific Gravity 0.970 g/cc
0.970 g/cc
Shin-Etsu Silicones KMP-400 Fluid
Information Provided by Shin-Etsu Silicones of America, Inc.
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
Teknor Apex Medalist® MD-225 Thermoplastic Elastomer
Uses: Medical/Healthcare Applications; Pharmaceuticals; Safety Equipment Agency Ratings: ISO 10993 Part 5 Processing Method: Extrusion; Injection Molding Forms: Pellets Injection Notes: Drying is no..
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
Teknor Apex TEKBOND® MP 1726 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
A. Schulman POLYFORT™ 1602 UV-3120 UV Stabilized, Glass Reinforced Copolymer Polypropylene
DescriptionPolyfort® FPP 1602 UV-3120 is a black UV stabilized 10% chemically coupled glass reinforced copolymer polypropylene.Information provided by A. Schulman.
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP 1602 Glass Reinforced, Chemically Coupled Homopolymer
DescriptionPolyfort® FPP 1602 is a 10% glass reinforced chemically coupled homopolymer.Information provided by A. Schulman.
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D 792
RTP Company RTP 101 CC HI Polypropylene (PP), High Impact - Glass Fiber - Chemically Coupled
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP 1602 Glass Reinforced, Chemically Coupled Homopolymer
DescriptionPolyfort® FPP 1602 is a 10% glass reinforced chemically coupled homopolymer.Information provided by A. Schulman.
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP1666 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1666 is a 10% talc filled homopolymer polypropylene compound. Information provided by A. Schulman.
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D 792
RTP Company ESD A 100 HF Polypropylene (PP); ESD Protection - Static Dissipative - High MFR
Specific Gravity 0.970 g/cc

@Temperature 25.0 °C
0.970 g/cc

@Temperature 77.0 °F
Dow Corning SYL-OFF® 7610 COATING
Syl-Off® 7610 Coating is a 100% active solids, pre-catalysed, coating containing a medium viscosity vinyl endblocked and pendant functional silicone polymer. General purpose coating with exceptiona..
Specific Gravity 0.970 g/cc

@Temperature 25.0 °C
0.970 g/cc

@Temperature 77.0 °F
Dow Corning SYL-OFF® PMCP7610 Coating
Syl-Off® 7610 Coating is a 100% active solids, pre-catalysed, coating containing a medium viscosity vinyl endblocked and pendant functional silicone polymer. General purpose coating with exceptiona..
Specific Gravity 0.970 g/cc

@Temperature 25.0 °C
0.970 g/cc

@Temperature 77.0 °F
Dow Corning SYL-OFF® PMCPSL 9156 Release Modifier
Syl-Off® SL 9156 Release Modifier is one component of a multi-component silicone release system designing for coating on polyester substrates.Information provided by Dow Corning
Specific Gravity 0.970 g/cc

@Temperature 25.0 °C
0.970 g/cc

@Temperature 77.0 °F
Dow Corning SYL-OFF® SL 160 COATING
Example of a typical SL 100/SL 200 blend; low release at high speeds; medium-low viscosityInformation provided by Dow Corning
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792 and ISO 1183
ExxonMobil Santoprene® 101-55W255 Thermoplastic Vulcanizate
Product Description: A soft, black thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material is designed for use in residential dishwasher applications and contains..
Specific Gravity 0.970 g/cc
0.970 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 271-64 Thermoplastic Elastomer
A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t..
Specific Gravity 0.970 g/cc
0.970 g/cc
Part B
Epoxy Technology EPO-TEK® 730 Unfilled Thermally and Electrically Insulating Epoxy
Material Description: A two component, room temperature-curing, thermally and electrically insulating epoxy. It can be used for adhesive, sealing, potting or encapsulation applications found in sem..
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
Asahi Kasei Thermylene® P-10FG-2100 10% Glass Fiber Reinforced
Information provided by Asahi Thermofil
Specific Gravity 0.970 g/cc
0.970 g/cc
"A" component
ACC QGel 300 QSI Quantum Silicones High Strength Gel
QGel 300 is a clear, very soft, tough, moderately cross-linked, silicone polymer. Silicone gels are used to provide protection from vibration, thermal or mechanical shock. Silicone gels also provide..
Specific Gravity 0.970 - 0.990 g/cc
0.970 - 0.990 g/cc
ASTM D792
Buckeye Polymers BP RPP 1209 GR BLK Polypropylene, 12% Glass Filled
Product Information: 12% glass reinforced polypropyleneProduct Features:Offers improved flex modulus while maintaining a low specific gravity propertyOffers improved heat stability and scratch and m..
Specific Gravity 0.970 g/cc
0.970 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 211-55 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Specific Gravity 0.970 g/cc
0.970 g/cc
23°C; ASTM D792
ExxonMobil Santoprene® 211-64 Thermoplastic Elastomer  (discontinued **)
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP 1602 Glass Reinforced, Chemically Coupled Homopolymer
DescriptionPolyfort® FPP 1602 is a 10% glass reinforced chemically coupled homopolymer.Information provided by A. Schulman.
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
A. Schulman POLYFORT™ FPP 1609 Mica Fortified Copolymer Polypropylene
DescriptionPolyfort® FPP 1609 is a 10% mica fortified copolymer polypropylene product. Information provided by A. Schulman.
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D 792
RTP Company RTP 2800 B-55A Thermoplastic Polyolefin Elastomer (TEO)  (discontinued **)
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Specific Gravity 0.970 g/cc
0.970 g/cc
ASTM D792
RTP Company RTP 2800B-50D HF  Thermoplastic Vulcanizate Elastomer (TPV) 50 Shore D - High Flow &n
50 Shore D - High FlowComments:50-D DurometerHigh FlowUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.Information provided by RT..