Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2.90 MPa | 420 psi | 200%, post cured- 4 hours at 204°C |
Multibase SILASTIC® C7-4550 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 2.90 MPa | 421 psi | ASTM D412 |
Polymax® Maxelast® A9730 TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Strength, Yield | 2.90 MPa | 421 psi | ASTM D412 |
Polymax® Maxelast® P2955T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 2.90 MPa | 421 psi | M100 |
3M Dyneon™ Aflas® FA-150L PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |
|||
Tensile Strength, Yield | 2.90 MPa | 421 psi | Support Sponge |
Fujipoly Industries Zebra® 1002 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 2.90 MPa | 421 psi | Support Sponge |
Fujipoly Industries Zebra® 1002 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 2.90 MPa | 421 psi | Support Sponge |
Fujipoly Industries Zebra® 2004 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 2.90 MPa | 421 psi | Support Sponge |
Fujipoly Industries Zebra® 2005 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 2.90 MPa | 421 psi | Support Sponge |
Fujipoly Industries Zebra® 2005 Carbon Sponge Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 2.90 MPa | 421 psi | Support Sponge |
Fujipoly Industries Zebra® LT 200 Low Temperature Carbon Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 2.90 MPa @Strain 100 % |
421 psi @Strain 100 % |
ASTM D412 |
LG Chemical KEYFLEX TO-1088A Thermoplastic Olefin for Injection Molding, 88A Hardness KEYFLEX resins, thermoplastic elastomers divided by polyester and polyolefin type, have been developed by LG`s own polymerization and compounding technology. They display the flexibility of rubber .. |
|||
Tensile Strength, Yield | 2.90 MPa | 420 psi | @50% Elongation; ASTM D1414 |
Greene Tweed CHEMRAZ® 605 Perfluoroelastomer Chemraz® 605, a perfluoroelastomer, is ideally suited for challenging fluid handling applications. A high temperature compound with superior compression set resistance, physical properties and e.. |
|||
Tensile Strength, Yield | 2.90 MPa | 421 psi | Support Sponge |
Fujipoly Industries Zebra® 2004 Carbon Solid Self-Supported Connectors Fujipoly Carbon Zebra Connectors and Low Temperature Carbon Zebra Connectors consist of alternating layers of conductive carbon filled and non-conductive silicone rubber. Contact density of the carb.. |
|||
Tensile Strength, Yield | 2.90 MPa | 420 psi | at 100%; ASTM D412 |
Multibase Multi-Flex® A 7321 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantUV Resistance, Good Processability, Good.. |
|||
Tensile Strength, Yield | 2.90 MPa | 420 psi | 100%; ASTM D412 |
Teknor Apex APEX® 3060-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tensile Strength, Yield | 2.90 MPa @Strain 100 % |
421 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5065UI Soft Touch Polyolefin Thermoplastic ApplicationInvision™ VX-5065UI is targeted for automotive injection molding appearance applications. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 2.90 MPa @Strain 100 % |
421 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5065UI Soft Touch Polyolefin Thermoplastic ApplicationInvision™ VX-5065UI is targeted for automotive injection molding appearance applications. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 2.90 MPa @Strain 100 % |
421 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5065UI Soft Touch Polyolefin Thermoplastic ApplicationInvision™ VX-5065UI is targeted for automotive injection molding appearance applications. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 2.90 MPa @Strain 100 % |
421 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5065UI Soft Touch Polyolefin Thermoplastic ApplicationInvision™ VX-5065UI is targeted for automotive injection molding appearance applications. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 2.90 MPa @Strain 100 % |
421 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5065UI Soft Touch Polyolefin Thermoplastic ApplicationInvision™ VX-5065UI is targeted for automotive injection molding appearance applications. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 2.90 MPa @Strain 100 % |
421 psi @Strain 100 % |
ISO 527 |
A. Schulman INVISION™ VX-5065UI Soft Touch Polyolefin Thermoplastic ApplicationInvision™ VX-5065UI is targeted for automotive injection molding appearance applications. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 2.90 MPa @Strain 100 % |
421 psi @Strain 100 % |
|
Daikin DAI-EL G-555 Fluoroelastomer Terpolymer, Bisphenol Curable Grade, 69% Fluorine Content Offers minimal compression set and excellent sealing. The terpolymer type is able to withstand polarized solvents to realize a wide range of application.Features: Products with excellent balance of.. |
|||
Tensile Strength, Yield | 2.90 MPa @Strain 50.0 % |
421 psi @Strain 50.0 % |
50 mm/min |
Arkema Group Pebax® 2533 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 25 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Tensile Strength, Yield | 2.90 MPa | 421 psi | cured for 72 hrs @ RT |
ACC QM 118 QSI Quantum Silicones 18 Durometer Condensation Cured Moldmaking Material QM 107 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Tensile Strength, Yield | 2.90 MPa | 421 psi | cured 72 hrs @ RT |
ACC QM 230F QSI Quantum Silicones 30 Durometer Addition Cure Moldmaking Material QM 230F is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for t.. |
|||
Tensile Strength, Yield | 2.90 MPa @Strain 100 % |
420 psi @Strain 100 % |
across flow; ASTM D412 |
ExxonMobil Santoprene® 8271-80HT Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer which complies with FDA regulations for rubber articles intended for repeated use. It can be processed using injection molding or extrusion melt pro.. |
|||
Tensile Strength, Yield | 2.90 MPa | 420 psi | at 100%; ASTM D412 |
PB1100-75 Polyurethane-based Biomedical Elastomer |