Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Specific Gravity = 1.32 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
PolyOne Geon™ Vinyl Packaging 2121 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
PolyOne Geon™ Vinyl Rigid Molding M5731 Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. Dark colored compounds do not..
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
PolyOne Geon™ Vinyl Wire & Cable WEMB410U Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
PolyOne Geon™ Vinyl Flexible R7661A Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Specific Gravity 1.32 g/cc
1.32 g/cc
Sylvin Technologies 8925-80 Natural PVC Extrusion Compound
Information provided by Sylvin Technologies Inc.
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
SABIC Innovative Plastics ULTEM UC1200 PEI (Asia Pacific)
12% carbon fiber reinforced Polyetherimide (Tg 217C). ECO Conforming. UL94 V0 listing in recognized colors.
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Teknor Apex APEX® 82_E254V-14 Polyvinyl Chloride, Flexible
Notes: 80°C Jacket; RoHS CompliantForms: PelletsInformation Provided by Teknor Apex
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Teknor Apex APEX® 90-A529C-72 Polyvinyl Chloride, Flexible
Notes: 80°C Jacket; RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex
Specific Gravity 1.32 g/cc
1.32 g/cc
23°C; ASTM D792
Teknor Apex APEX® 94-A0098A-60 Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose Uses-General PurposeAppearance-Natural Color, OpaqueForms-PelletsProcessing Method-I..
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Teknor Apex Flexalloy® 9605-70FR Polyvinyl Chloride, Elastomer
Notes: 105°C Jacket; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility; Sunlight Resistant (720 hours) Uses Cable Jacketing Wire Types: SEOW; SEW; SJEOW;..
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Teknor Apex Sinpolene GPP1640 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 40% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; ..
Specific Gravity 1.32 g/cc
1.32 g/cc
ISO 1183/1
A. Schulman SCHULAMID® 6 GB30 30% Glass Bead Reinforced Nylon 6
Information provided by A. Schulman.
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
A. Schulman POLYBATCH™ Green 3011E Concentrate Based In Polyethylene
DescriptionPOLYBATCH® 3011E is a green color concentrate based in polyethylene. This concentrate was designed to provide color in polyolefin film and molding applications. POLYBATCH® 3011E is he..
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
A. Schulman POLYBATCH™ Brown 10305U Concentrate Based In LLDPE
DescriptionPOLYBATCH® 10305U is a brown color concentrate containing optimized blend of color and UV based in LLDPE. This concentrate was designed to provide color and UV stability in polyolefin p..
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
A. Schulman POLYBATCH™ Blue 40395U Concentrate Based In LLDPE
DescriptionPOLYBATCH® 40395U is a blue color concentrate containing an optimized blend of color and UV stabilizer based in LLDPE. This concentrate was designed to provide color and UV stability in..
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Eastman Eastar EN067 Copolyester, Natural
Eastar Copolyester EN067 is a copolymer PET with good color. This product is supplied as a crystalline pellet that has improved flowability characteristics. Due to slower crystallization kinetics, t..
Specific Gravity 1.32 g/cc
1.32 g/cc
ISO 2781
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Extrusion, Natural
Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and..
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
DuPont Performance Polymers VESPEL TP-8169 Polyimide
DuPont Vespel TP-8169 parts are specified for high-temperature applications. TP-8169 parts offer a unique balance of mechanical and thermal properties for high performance in aggressive environments..
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
E-Polymers SEPAZ® V215A 15% Glass Fiber Reinforced PPA
Polyphthal Amide Resin (High Temperature Nylon): SEPAZ PPA is a unique semi-crystalline engineering plastic that bridges the cost-performance gap between traditional engineering thermoplastics and s..
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Colorite Polymers 1066 Non-Phthalate 66 Series Vinyl Compound
Description: The Colorite 66 series is a family of non-toxic PVC compounds developed specifically for those medical device, food, and infant care items for which the use of a citrate* based non-phth..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 15642 Wire & Cable Flexible PVC
Non-lead stabilized semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C.Information provided by Georgia GulfGeorgia Gulf became Axiall Cor..
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D-792
Axiall 7020 Rigid PVC, Extrusion
Georgia Gulf 7020 is a special purpose rigid PVC profile extrusion compound designed for thin-wall applications requiring the following properties: Impact Strength & ToughnessDimensional StabilityF..
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D-792
Axiall 9209 Rigid PVC, Molding
Georgia Gulf 9209 is a food grade compound containing excellent optical and processing characteristics. It is suitable for use in a variety of food, cosmetic and general purpose packaging applicati..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 11441 Wire & Cable Flexible PVC
Clear extrusion compound formulated for applications necessitating a high degree of flame retardancy.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Specific Gravity 1.32 g/cc
1.32 g/cc
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled
These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F.
Specific Gravity 1.32 g/cc
1.32 g/cc
Aremco Corr-Paint™ CP4095 High Temperature Protective Coating Silicone, Aluminum Filled
This silicone-based, heat resistant coatings are formulated using a state-of-the-art, VOC-compliant, water-dispersible silicone resin. CP4000 adheres to metals, ceramics, refractories, and quartz, a..
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D-792
Axiall 9017J Clear 06 Rigid PVC, Molding, Clear
Georgia Gulf 9017J Clear 06 is for food packaging and personal care applications requiring optimum taste and odor properties. The compound contains an ultraviolet light stabilizer, which protects l..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 18840 Wire & Cable Flexible PVC
Non-lead stabilized 105C jacket compound for use in SPTO, SJTO and SVTO applications. Best suited for 30 mil walls and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat..
Specific Gravity 1.32 - 1.36 g/cc
1.32 - 1.36 g/cc
ASTM D-792
Axiall 8918 Moldings & Extrusions Flexible PVC
Non-lead migration resistant extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.