Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer A. Schulman, Inc.
Trade Name POLYTROPE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dimensional stability. TPP 293 is UV stable and pigmentable.ApplicationTypical applications include bumper rubstrips and step pads. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Linear Mold Shrinkage 0.0090 - 0.011 cm/cm
0.0090 - 0.011 in/in
Melt Index of Compound 5.0 g/10 min
5.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
ASTM D2240
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D638
Elongation at Break 550 %
550 %
ASTM D638
Flexural Modulus 0.586 GPa
85.0 ksi
ASTM D790
Gardner Impact 36.0 J

@Temperature -30.0 °C
26.6 ft-lb

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Brittleness Temperature -45.0 °C
-49.0 °F