Thermal Properties | Metric | English | Comments |
---|---|---|---|
Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WJB593KBL Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
PolyOne Geon™ Vinyl Wire & Cable WR7426L Polyvinyl Chloride, Flexible (PVC, Flexible) Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provide.. |
|||
Brittleness Temperature | -45.0 - -40.0 °C | -49.0 - -40.0 °F | Average value: -43.3 °C Grade Count:3 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Blow Molding Grade". Each property range of values reported is m.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
Eastman 18BOA Polyethylene
(discontinued **) Polyethylene 18BOA is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on automatic mold.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
Eastman 811P Polyethylene
(discontinued **) Injection grade. With its high melt index, the material flows well in molding machines and fills large molds with ease. It is used for molding housewares and other items where a flexible, easy mol.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
Eastman D4044A Polyethylene
(discontinued **) D4044-A is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on automatic molding equipme.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
Eastman Voridian D4053-A Polyethylene
(discontinued **) Voridian polyethylene D4053-A is a low density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easily on aut.. |
|||
Brittleness Temperature | <= -45.0 °C | <= -49.0 °F | |
Sibur 1045-12 Compound 948 Polyvinyl Chloride (PVC) Shall correspond to control sample, approved in accordance with the established procedure. Pores, which can be seen by eyes, are not allowed. Plastic shall no burn at stop of worm extruder for a p.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
Teknor Apex APEX® 1700-55 Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-General Purpose, Low Gloss Uses-Appliance Components, Footwear, FurnitureForms-PelletsProcessing Met.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 89501-83FR Polyvinyl Chloride, Elastomer Notes: 105°C Insulation; RoHS Compliant Features: High Heat Resistance; Low Temperature Flexibility Uses Wet Rated Insulation Wire Types: NISPE-1; NISPE-2; SE; SEO; SEOW; SEW; SJE; SJEO; SJEOW; S.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
Teknor Apex Flexalloy® 9900-55 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and .. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
Teknor Apex APEX® 07-U0296A-65 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ CB 1010U-330 Injection Molding Reactor Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope CB 1010U-330 is a color matched/color blended injection molding reactor grade olefinic thermoplastic elastomer (TPO). This product has excellent low temperature impact properti.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ TPP 403 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 403 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | Cold Flex; ISO 458/2 |
Fainplast Compounds GA 63 Flexible PVC, Flame Retardant Sheathing Good flexibility |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D746 |
Colorite Polymers Weatherflex™ CS1534WX (NTL02P) Wire and Cable Vinyl Compound Description: Colorite specialty wire and cable compounds feature low smoke properties, excellent flame retardance, low temperature flexibility, and resistance to abrasion and chemicals. All are avai.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D-746 |
Axiall 67441 Wire & Cable Flexible PVC 90°C rated, non-lead stabilized, inner/outer jacketing compound meets -40°C low temp impact and FT4 flame requirements in Teck 90 cables. Low acid gas 12%-13% per CSA test methods. Meets CSA 22... |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | ASTM D-746 |
Axiall 8651 Moldings & Extrusions Flexible PVC A quality, low gravity extrusion compound with excellent low temperature properties. Designed for use in weatherstrips, flexible gaskets and extruded shapes.Information provided by Georgia GulfGeor.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ TPP 510 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 510 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Brittleness Temperature | -45.0 °C | -49.0 °F | |
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim.. |