Polymer Property : Flexural Modulus = 85.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.586 GPa
85.0 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers NPP 50-0548
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Flexural Modulus 0.586 GPa
85.0 ksi
ASTM D790
Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet)
Flexural Modulus 0.586 GPa
85.0 ksi
ASTM D790
Quadrant EPP TIVAR® SuperPlus UHMW-PE, Glass-filled Cross-linked & Heat Stabilized Extreme Wear Resistant (ASTM Product Data Sheet)
Flexural Modulus 0.586 - 2.62 GPa
85.0 - 380 ksi
Average value: 1.24 GPa Grade Count:214
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Blow Molding Grade". Each property range of values reported is minimum..
Flexural Modulus 0.586 GPa
85.0 ksi
ASTM D790
Global TPO-55D TPO Grade
Data provided by Global Polymers Corporation.
Flexural Modulus 0.586 GPa
85.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim..
Flexural Modulus 0.586 GPa
85.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene
Information provided by A. Schulman.
Flexural Modulus 0.586 GPa
85.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim..
Flexural Modulus 0.586 GPa
85.0 ksi
ASTM D790
Chase Plastics CP Pryme® NN300STL (COND, 50% RH) Nylon 66 (Utility Grade), Super Toughened, Internally Lubricated
Information provided by Chase Plastics.
Flexural Modulus 0.586 GPa
85.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene
Information provided by A. Schulman.
Flexural Modulus 0.586 GPa
85.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim..
Flexural Modulus 0.586 GPa
85.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene
Information provided by A. Schulman.
Flexural Modulus 0.586 GPa
85.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim..
Flexural Modulus 0.586 GPa
85.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene
Information provided by A. Schulman.
Flexural Modulus 0.586 GPa
85.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene
Information provided by A. Schulman.
Flexural Modulus 0.586 GPa
85.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim..
Flexural Modulus 0.586 GPa
85.0 ksi
at 1% secant modulus; ASTM D790
A. Schulman POLYAXIS® RLLP621 Flame Retardant, High Density Polyethylene
Information provided by A. Schulman.
Flexural Modulus 0.586 GPa
85.0 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 293 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP293 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring excellent low temperature impact properties with good dim..