Material Notes:
Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 96%Stress Relaxation after 1000 hrs @ 200°C: 75%Formability Ratio, 90° Bend, Radius/Thickness (Good Way): 1.5Formability Ratio (bad Way): 1.5Superficial Hardness: 30T 82-89Brush 60™ is a new generation, high conductivity copper beryllium alloy which is specifically engineered to meet the stringent electrical and mechanical requirements of computer, datacom, and telecommunications applications. Performance benefits include:Signal reliabilityDurabilityDesign flexibilityManufacturabilityRecyclabilityBrush Engineered Materials Inc. changed its name to Materion Corporation in March 2011.
Physical Properties Metric English Comments
Density 8.80 g/cc
0.318 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 99 - 106
99 - 106
Tensile Strength, Ultimate 825 - 965 MPa
120000 - 140000 psi
Tensile Strength, Yield 720 - 860 MPa
104000 - 125000 psi
Elongation at Break >= 10 %
>= 10 %
Modulus of Elasticity 138 GPa
20000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.0 µm/m-°C

@Temperature 20.0 - 200 °C
10.0 µin/in-°F

@Temperature 68.0 - 392 °F
Thermal Conductivity 221 W/m-K
1530 BTU-in/hr-ft²-°F
Melting Point 1030 - 1080 °C
1890 - 1980 °F
Solidus 1030 °C
1890 °F
Liquidus 1080 °C
1980 °F
Component Elements Properties Metric English Comments
Beryllium, Be 0.15 - 0.50 %
0.15 - 0.50 %
Copper, Cu 98.1 %
98.1 %
as balance
Nickel, Ni 1.0 - 1.4 %
1.0 - 1.4 %
Tin, Sn <= 0.25 %
<= 0.25 %
Zirconium, Zr <= 0.50 %
<= 0.50 %
Electrical Properties Metric English Comments
Electrical Resistivity <= 0.00000340 ohm-cm
<= 0.00000340 ohm-cm
50% IACS conductivity (minimum)
Users viewing this material also viewed the following: