Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Hiloy® 164 Polypropylene, Mineral Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer A. Schulman ComAlloy
Trade Name Hiloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Hiloy® 164 Polypropylene, Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ASTM D785
Tensile Strength, Ultimate 19.0 MPa
2760 psi
ASTM D638
Elongation at Break 6.1 %
6.1 %
ASTM D638
Flexural Strength 46.0 MPa
6670 psi
ASTM D790
Flexural Modulus 6.00 GPa
870 ksi
ASTM D790
Izod Impact, Notched 0.270 J/cm
0.506 ft-lb/in
ASTM D256
Izod Impact, Unnotched 1.33 J/cm
2.49 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 143 °C
289 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °C
198 °F
ASTM D648
Processing Properties Metric English Comments
Middle Barrel Temperature 210 - 221 °C
410 - 430 °F
Copyright © lookpolymers.com All Rights Reserved