Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT1055-624 Thermoplastic Polyolefin, Non-UV Stabilized, General Purpose Light Grey Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT1055-685UV Thermoplastic Polyolefin, UV Stabilized, Graphite Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT3080-50 Thermoplastic Polyolefin, UV Stabilized, YGYA Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products FT3080-729UV Thermoplastic Polyolefin, UV Stabilized, AG-64 Grey Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP513-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P104-00 Polypropylene, Natural Applications: Consumer goodsIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P107-00 Polypropylene Homopolymer, Natural Applications: Wire harnessesTrim componentsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P250-00 Polypropylene Copolymer, Natural Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P251-00 Polypropylene Copolymer, Natural Applications: Fuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P252-00 Polypropylene Copolymer, Natural Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P252-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P256-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P257-00 Polypropylene Copolymer, Natural Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P261-01 Polypropylene Copolymer, Medium Impact, Black Applications: Radiator grille inlet supportElectrical housingsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products P601-01 Polypropylene Copolymer, Black Applications: Engine componentChassis componentConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 379 - 430 °F | |
PolyOne Versaflex™ CL2242 Thermoplastic Elastomer (TPE) Versaflex™ CL2242 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Ravago Manufacturing Americas Hylac® HF143 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Ravago Manufacturing Americas Hylac® HF96 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black Applications: Automotive interior applicationsSeat back trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 193 - 221 °C | 380 - 430 °F | |
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced Acrylonitrile Butadiene Styrene, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Middle Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
Polymer Resources ABS-G25 ABS, 25% Glass Reinforced Acrylonitrile Butadiene Styrene, 25% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Middle Barrel Temperature | 204 - 221 °C | 400 - 430 °F | |
PTS SAN-82TR SAN Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 199 - 221 °C | 390 - 430 °F | |
Multibase Multi-Flex® D 3104-8 TPO Thermoplastic Polyolefin Elastomer Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot.. |
|||
Middle Barrel Temperature | 213 - 221 °C | 415 - 430 °F | |
Teknor Apex Telcar® TL-8421 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Middle Barrel Temperature | 213 - 221 °C | 415 - 430 °F | |
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;.. |
|||
Middle Barrel Temperature | 213 - 221 °C | 415 - 430 °F | |
Teknor Apex Telcar® TL-8730 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou.. |
|||
Middle Barrel Temperature | 210 - 221 °C | 410 - 430 °F | |
A. Schulman ComAlloy Comtuf® 164 Polypropylene, Mineral Reinforced, Chemically Coupled, Impact Modified Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |