Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 6670 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 46.0 MPa
6670 psi
ASTM D790
Proto3000 Duraform® EX Selective Laser Sintering (SLS®) Prototyping Polymer
Plastic for use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systemsDescription: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and..
Flexural Strength <= 46.0 MPa
<= 6670 psi
ISO 178
Polykemi AB POLYfill PP HIP16020FCF Polypropylene, Fast Cycle
Information provided by Polykemi AB
Flexural Strength <= 46.0 MPa
<= 6670 psi
ISO 178
Polykemi AB POLYfill PPC T20040 Polypropylene Copolymer, Mineral Reinforced
Information provided by Polykemi AB
Flexural Strength <= 46.0 MPa
<= 6670 psi
ISO 178
Polykemi AB POLYfill PPH TS2020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Flexural Strength <= 46.0 MPa
<= 6670 psi
ISO 178
Polykemi AB POLYfill PPH TS4020D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant
Information provided by Polykemi AB
Flexural Strength 46.0 MPa
6670 psi
Reliance Industries Polypropylene - Wollastonite filled
Information provided by Reliance Industries
Flexural Strength 46.0 MPa
6670 psi
ASTM D790
Ineos Nova Zylar® 533 Clear Impact Modified UV Stabilized Acrylic Copolymer  (discontinued **)
Features: High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationExcellent indoor light stabilityHigh elongation and ductilityApplications: Appliance..
Flexural Strength 46.0 MPa
6670 psi
at 3.5% strain; ISO 178
FKuR Kunststoff Bio-Flex® S 5630 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Flexural Strength 46.0 MPa
6670 psi
ASTM D790
LG Chemical LUPOL GP-3154F General Purpose Polypropylene, 15% Mineral Fillers, High Modulus, Flame Retardant
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner..
Flexural Strength 46.0 MPa
6670 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Lubricomp ML003 PP (Europe-Africa-Middle East)
LNP* Lubricomp* ML003 is a compound based on Polypropylene resin containing PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Strength 46.0 MPa
6670 psi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON AX01706 ABS
LNP* STAT-KON* AX01706 is a compound based on ABS containing proprietary fillers. Added feature of this grade is: Electrically Conductive.
Flexural Strength 46.0 MPa
6670 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP MB006S PP
LNP THERMOCOMP* MB006S is a compound based on Polypropylene resin containing 30% Glass Bead. Added features of this material include: Heat Stabilized.
Flexural Strength 46.0 MPa
6670 psi
ISO 178
Styrolution PS 416N HIPS
Styrolution PS 416N is medium impact polystyrene with very good flow properties. It has a high rigidity whilst displaying a very good surface gloss.Very good flow propertiesHigh rigidityVery good su..
Flexural Strength 46.0 MPa
6670 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-LOY KX95702 Acetal
LNP STAT-LOY* KX95702 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Antistat.
Flexural Strength 46.0 MPa
6670 psi
ISO 178
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
Flexural Strength 46.0 MPa
6670 psi
ISO 178
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific)
LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact.
Flexural Strength 46.0 MPa
6670 psi
ASTM D790
Eastman Tenite 383A2R30010 Cellulose Acetate Propionate, Natural, Trsp
Applications:Oral HygienePlastics for hygiene feminine productsRecreationalToothbrushesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughne..
Flexural Strength 46.0 MPa
6670 psi
ASTM D790
Entec Hypro™ PPC-T40 Copolymer Polypropylene, 40% Talc Reinforced
Information provided by Entec
Flexural Strength 46.0 MPa
6670 psi
ASTM D790
Aclo Accutech Polypropylene Homopolymer HP0336M20CL Mica Reinforced Coupled
Flexural Strength 46.0 MPa
6670 psi
ISO 178
Azoty Tarnow™ TARNOFORM 300 HI2 POM
Rubber modified grade with very high impact strength and damping capacity.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Flexural Strength 46.0 MPa
6670 psi
XY direction; ASTM D790
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer
Unfilled PA 11 formulated for easy processing. Can be run as a drop-in replacement for other commercially available PA 11 laser sintering powders. Parts produced from PA 850 exhibit outstanding mech..
Flexural Strength 46.0 MPa
6670 psi
ASTM D790
A. Schulman ComAlloy Hiloy® 164 Polypropylene, Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Strength 46.0 MPa
6670 psi
ASTM D790
Aclo Accutech Polypropylene Copolymer CP0436G10M20CL Glass/Mineral Reinforced Coupled
Flexural Strength 46.0 MPa
6670 psi
Plastcom SLOVALEN PH 72 T 20 PP, 20% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh..
Flexural Strength <= 46.0 MPa
<= 6670 psi
ISO 178
Polykemi AB POLYfill PPC GF5020 Polypropylene Copolymer, Glass Fiber Reinforced
Information provided by Polykemi AB
Flexural Strength <= 46.0 MPa
<= 6670 psi
ISO 178
Polykemi AB POLYfill PPH TS3020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Flexural Strength <= 46.0 MPa
<= 6670 psi
ISO 178
Polykemi AB POLYfill PPH TS4020 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Flexural Strength 46.0 MPa
6670 psi
ASTM D790
Ineos Nova Zylar® 530 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:High clarityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationMeets USP XXIII specifications for Class VI plasticsUL94 HB @ 1.5 mm for uncolored ma..
Flexural Strength 46.0 MPa
6670 psi
ASTM D790
Ineos Nova Zylar® 535 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features: High clarity, strength and toughnessStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationAnti-stat packageEnhanced mold releaseUL 94HB @ 1.5 mm for a..
Flexural Strength 46.0 MPa
6670 psi
ISO 178
Polyplastic Armlen® PP MD 40-4HS-901 Polypropylene, 40% Mineral Filled
Heat stabilizedInformation provided by PolyPlastic Group.
Copyright © lookpolymers.com All Rights Reserved