Polymer Property : Middle Barrel Temperature = 221 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT2500-594UV Thermoplastic Polyolefin, UV Stabilized, 9428NM Spectra Grey
Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT2600-01UV Thermoplastic Polyolefin, UV Stabilized, Black
Applications: Interior trimSplash shieldsStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT2700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Air deflectorsFuel filler shieldsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products FT3080-640UV Thermoplastic Polyolefin, UV Stabilized, BFQA Arizona Beige
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP513-01 High Stiffness Polypropylene Copolymer, Medium Impact, UV Stabilized, Black
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P100-00 Polypropylene, Natural
Applications: Automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P100-01 Polypropylene Homopolymer, Black
Applications: Wire harnessesTrim componentsUnderhood applicationsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P249-01UV General Purpose Polypropylene Copolymer, UV Stabilized, Black
Applications: LP bracketsSplash shieldsDoor/trunk scuffInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P250-00 Polypropylene Copolymer, Natural
Applications: ConsolesComponent housingsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P252-00 Polypropylene Copolymer, Natural
Applications: Interior trimUnderhood componentsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P252-01 Polypropylene Copolymer, Black
Applications: Cowl screenInterior trimBumper coverGlove box binInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P252-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P254-01 Polypropylene Copolymer, Black
Applications: Air ducts - distributionFuse panel coversSplash shieldsElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products P256-762 Polypropylene Copolymer, Medium Grey
Applications: Misc. ClipsElectrical housingInjection molding conditions reported in table.Information provided by RheTech Products.
Middle Barrel Temperature 210 - 221 °C
410 - 430 °F
Polymer Resources ABS-G10 ABS, 10% Glass Reinforced
Acrylonitrile Butadiene Styrene, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Middle Barrel Temperature 210 - 221 °C
410 - 430 °F
Polymer Resources ABS-G5 ABS, 5% Glass Reinforced
Acrylonitrile Butadiene Styrene, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information ..
Middle Barrel Temperature 210 - 221 °C
410 - 430 °F
Polymer Resources ABS-G5-[color]-3 ABS, 5% Glass Reinforced, UV-stabilized
Acrylonitrile Butadiene Styrene, 5% Glass Reinforced, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl..
Middle Barrel Temperature 199 - 221 °C
390 - 430 °F
Ravago Manufacturing Americas Hylac® GP74 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Middle Barrel Temperature 210 - 221 °C
410 - 430 °F
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced
Acrylonitrile Butadiene Styrene, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Middle Barrel Temperature 210 - 221 °C
410 - 430 °F
Polymer Resources ABS-G25 ABS, 25% Glass Reinforced
Acrylonitrile Butadiene Styrene, 25% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information..
Middle Barrel Temperature 199 - 221 °C
390 - 430 °F
Ineos Nova Zyntar® F7080UV Developmental Flame Retardant Polystyrene  (discontinued **)
Features: General purpose non-Deca based resin (does not combine with Decabromodiphenyloxide)Good indoor UV light color stability(grey colors)UL94 V-0 @ 1.5 mm for all colors Good aesthetics for inj..
Middle Barrel Temperature 204 - 221 °C
400 - 430 °F
Fiberfil® J-60/GB/20 Polypropylene Homopolymer, 20% Glass beads
Information provided by FIBERFIL Engineered Plastics
Middle Barrel Temperature 199 - 221 °C
390 - 430 °F
Multibase Multi-Flex® D 5308 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, GoodScratch Resistant Forms:PelletsProcessing Method:Injection Molding Uses: Automot..
Middle Barrel Temperature 199 - 221 °C
390 - 430 °F
Multibase Multi-Flex® D 6505 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone ResistantDensity, LowTear Strength, GoodUV Resistance, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsInform..
Middle Barrel Temperature 199 - 221 °C
390 - 430 °F
Multibase Multi-Flex® D 6606 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone ResistantDensity, LowTear Strength, GoodUV Resistance, GoodStiffness, Good Forms:PelletsUses: Automotive ApplicationsInformation provided by Mul..
Middle Barrel Temperature 199 - 221 °C
390 - 430 °F
Multibase Multi-Flex® 1047-0000 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI..
Middle Barrel Temperature 199 - 221 °C
390 - 430 °F
Multibase Multi-Flex® 1047-2000 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant Thermal Stability, GoodDensity, LowTear Strength, Good Forms:PelletsProcessing Method:Injection Molding Uses: Automotive ApplicationsI..
Middle Barrel Temperature 213 - 221 °C
415 - 430 °F
Teknor Apex Telcar® TL-8730 Thermoplastic Elastomer
Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Industrial Cable Jacketing; Terminal Cable Jacketing; Undergrou..
Middle Barrel Temperature 210 - 221 °C
410 - 430 °F
A. Schulman ComAlloy Hiloy® 164 Polypropylene, Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Middle Barrel Temperature 193 - 221 °C
380 - 430 °F
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products.