Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman ComAlloy Comshield® 229 ABS, Electrically Conductive - Stainless Steel Fiber Filled

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
Manufacturer A. Schulman ComAlloy
Trade Name Comshield®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Comshield® 229 ABS, Electrically Conductive - Stainless Steel Fiber Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Yield Strength 69.0 MPa
10000 psi
ASTM D790
Flexural Modulus 3.00 GPa
435 ksi
ASTM D790
Izod Impact, Unnotched 4.30 J/cm
8.06 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
219 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 0.100 - 1.00 ohm-cm
0.100 - 1.00 ohm-cm
Surface Resistance 1.0 - 10 ohm
1.0 - 10 ohm