Electrical Properties Metric English Comments
Electrical Resistivity 0.100 - 1.00e+10 ohm-cm
0.100 - 1.00e+10 ohm-cm
Average value: 2.95e+8 ohm-cm Grade Count:60
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Electrical Resistivity 0.100 - 1.00e+16 ohm-cm
0.100 - 1.00e+16 ohm-cm
Average value: 7.69e+15 ohm-cm Grade Count:13
Overview of materials for Styrenic TPE  (Unverified Data**)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic TPE". Each property range of values reported is minimum and maximum values of appropriate MatWe..
Electrical Resistivity 0.100 - 1.00e+14 ohm-cm
0.100 - 1.00e+14 ohm-cm
Average value: 4.62e+13 ohm-cm Grade Count:13
Overview of materials for Acetal Copolymer, Steel Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of..
Electrical Resistivity 0.100 - 1000 ohm-cm
0.100 - 1000 ohm-cm
Average value: 258 ohm-cm Grade Count:27
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu..
Electrical Resistivity 0.100 - 1.00e+12 ohm-cm
0.100 - 1.00e+12 ohm-cm
Average value: 1.58e+10 ohm-cm Grade Count:64
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
Electrical Resistivity 0.100 ohm-cm - 1e+05
0.100 ohm-cm - 1e+05
Average value: 1160 ohm-cm Grade Count:17
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet..
Electrical Resistivity 0.100 - 1.00e+8 ohm-cm
0.100 - 1.00e+8 ohm-cm
Average value: 1260 ohm-cm Grade Count:45
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Electrical Resistivity 0.100 - 1.00e+8 ohm-cm
0.100 - 1.00e+8 ohm-cm
Average value: 4.37e+6 ohm-cm Grade Count:26
Overview of materials for Nylon 612, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Carbon Fiber Filler". Each property range of values reported is minimum and maximum values of..
Electrical Resistivity 0.100 - 10.0 ohm-cm
0.100 - 10.0 ohm-cm
Average value: 5.39 ohm-cm Grade Count:4
Overview of materials for Nylon 11 + Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 + Carbon Fiber". Each property range of values reported is minimum and maximum values of approp..
Electrical Resistivity 0.100 - 25.0 ohm-cm
0.100 - 25.0 ohm-cm
MarkeTech Silicon Single Crystal Semiconductor Wafer, n-type, Phosphorous Doped, Czochralski-LED Grown
Data provided by the supplier, MarkeTech International.MarkeTech International supplies standard silicon single crystals grown with diameters from 51 to 150 mm from polycrystal material with donor c..
Electrical Resistivity <= 0.100 ohm-cm
<= 0.100 ohm-cm
specific resistance
Imerys Kaolexâ„¢ SC Kaolin
Kaolex SC is an air floated Hydrated Aluminum Silicate. It is a low surface area, low viscosity, medium casting filler/extender for ceramic applications.Information provided by Imerys
Electrical Resistivity 0.100 ohm-cm
0.100 ohm-cm
Through-Plane
GrafTech eGRAF® SPREADERSHIELD™ SS600 Graphite
Made from flexible graphite, eGRAF® SPREADERSHIELD™ products function as both a passive heat spreader and heat shield. SPREADERSHIELD™ material can be die-cut, press-formed, or laminate..
Electrical Resistivity 0.100 - 1.00 ohm-cm
0.100 - 1.00 ohm-cm
ASTM C611
Techmer ES Electrafil® DB-1200/S/7/FR ABS, 7% Stainless Steel Fiber Reinforced (dry blend), Flame Retardant
Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL..
Electrical Resistivity 0.100 - 1.00 ohm-cm
0.100 - 1.00 ohm-cm
ASTM C611
Techmer ES Electrafil® DB-1200/SS/7 ABS, 7% Stainless Steel Fiber Reinforced (dry blend)
Superior cost-performance when compared with other electrically conductive resins is a hallmark of Electrafil stainless steel fiber reinforced ABS. Electrafil compounds can be formulated to meet UL..
Electrical Resistivity 0.100 ohm-cm
0.100 ohm-cm
Specific Resistance
UBE Tyranno Grade H Ceramic Semi-Conductive Fiber
Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e..
Electrical Resistivity 0.100 - 0.500 ohm-cm
0.100 - 0.500 ohm-cm
Specific resistance
UBE Tyrannohex® Heat Resistant Composite
Description: Tyrannohex is a fiber assembled ceramic with both toughness like a shell or wood and excellent heat-resistance in air.Very high volume fraction (Vf) of the thin (~ 10m), continuous fibe..
Electrical Resistivity <= 0.100 ohm-cm
<= 0.100 ohm-cm
ASTM D1829
CoorsTek Pure SiC™ LR CVD Silicon Carbide, > 99.9995%
Data Provided by the manufacturer, CoorsTek, Inc.
Electrical Resistivity 0.100 - 1.00 ohm-cm
0.100 - 1.00 ohm-cm
A. Schulman ComAlloy Comshield® 229 ABS, Electrically Conductive - Stainless Steel Fiber Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Electrical Resistivity 0.100 - 10.0 ohm-cm
0.100 - 10.0 ohm-cm
Average value: 6.70 ohm-cm Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), NCG Fiber
This property data is a summary of similar materials in the MatWeb database for the category "PPS + NGG". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Electrical Resistivity 0.100 - 1.00e+10 ohm-cm
0.100 - 1.00e+10 ohm-cm
Average value: 2.94e+8 ohm-cm Grade Count:35
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Stainless Steel Fiber Filled". Each property range of values repo..
Electrical Resistivity 0.100 - 6.70e+17 ohm-cm
0.100 - 6.70e+17 ohm-cm
Average value: 2.85e+16 ohm-cm Grade Count:351
Overview of materials for Polyetherimide (PEI)
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat..