A. Schulman ComAlloy Comshield® 215 High Impact Polystyrene, Electrically Conductive - Carbon Black Filled

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Carbon Black Filled
Manufacturer A. Schulman ComAlloy
Trade Name Comshield®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman ComAlloy Comshield® 215 High Impact Polystyrene, Electrically Conductive - Carbon Black Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Ultimate 32.0 MPa
4640 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Strength 49.0 MPa
7110 psi
ASTM D790
Flexural Modulus 6.00 GPa
870 ksi
ASTM D790
Izod Impact, Unnotched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °C
189 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
Surface Resistance 1000 - 10000 ohm
1000 - 10000 ohm