Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | |
Chevron Phillips 7105T LLDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 214, A 35307Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Contain.. |
|||
Tensile Strength, Ultimate | 32.0 - 50.0 MPa @Temperature 60.0 - 120 °C |
4640 - 7250 psi @Temperature 140 - 248 °F |
Average value: 41.7 MPa Grade Count:1 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Tensile Strength, Ultimate | 32.0 MPa @Temperature 120 °C |
4640 psi @Temperature 248 °F |
ISO 527 |
LATI LATAN 13 G/15 15% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Tensile Strength, Ultimate | 32.0 - 75.8 MPa | 4640 - 11000 psi | Average value: 57.6 MPa Grade Count:15 |
Overview of materials for Cyclo Olefin Polymer This property data is a summary of similar materials in the MatWeb database for the category "Cyclo Olefin Polymer". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ISO 527 |
LATI LATAMID 12 H FE90 Nylon 12 Base Magnetizable Compound
(Unverified Data**) Description: These are compounds containing a high percentage of magnetizable fillers; compared to traditional techniques for the manufacture of magnets, this allows the molding of complex shapes us.. |
|||
Tensile Strength, Ultimate | 32.0 MPa @Temperature 22.0 °C |
4640 psi @Temperature 71.6 °F |
25mm flat samples, compression moulded; ISO 527-4 |
Menzolit Menzolit® BMC 1500 Unsaturated Polyester UP BMC 1500 is a special BMC for the use at elevated temperature. The glass content is set to a level that combines good flowability with good strength and stiffness properties. Even without a specific.. |
|||
Tensile Strength, Ultimate | 32.0 MPa @Temperature 1150 °C |
4640 psi @Temperature 2100 °F |
|
Haynes 214® alloy, cold rolled annealed sheet 2.0-3.2 mm thick Intended principally for use at temperatures of 955°C and above, exhibits resistance to oxidation that exceeds virtually all conventional heat-resistant wrought alloys. Applications include mesh .. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ASTM D638 |
Ineos ABS Triax® 1220 S ABS + Polyamide Blend, Extrusion, Conditioned Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ASTM D638 |
Ineos ABS TRIAX® 1220 S ABS/Nylon Blend, As Conditioned Extrusion and injection molding grade with good stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical dampi.. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ASTM D638 |
Plenco 5118 Phenolic, Granular, Compression Molded PLENCO 05118 is a mineral and graphite filled phenolic molding compound, formulated for bearing seals. 05118 provides for a low coefficient of friction, abrasion resistance, minimal water absorptio.. |
|||
Tensile Strength, Ultimate | 32.0 MPa @Temperature -20.0 °C |
4640 psi @Temperature -4.00 °F |
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638 |
DuPont Elvax® 660 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Tensile Strength, Ultimate | 32.0 MPa @Temperature -20.0 °C |
4640 psi @Temperature -4.00 °F |
Type IV, crosshead speed 2 in/min, at -20°C; ASTM D638 |
DuPont Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ASTM D638 |
Lubrizol Estaloc® 61225 Polyester-Type Thermoplastic Alloy Type: Estaloc® 61225 Alloy RETPU is a polyester-type thermoplastic alloy.Features: Fast cycling, dimensional stability, durability, aesthetics, low temperature impact.Uses: Injection molding.Availa.. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ASTM D412 |
Lubrizol Estane® 2103-85AE Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Film and profile resinAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in.. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | DIN 53504 |
Lubrizol ESTANE® 58561 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ISO 527-1 |
Dow BETAMATE™ 1496 V Epoxy BETAMATE™ 1496 V is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties: Good rheology performance (Wash-out resistant, excelle.. |
|||
Tensile Strength, Ultimate | 32.0 MPa @Temperature 816 °C |
4640 psi @Temperature 1500 °F |
|
AK Steel 409 ULTRA FORM® Stainless Steel AK Steel 409 ULTRA FORM Stainless Steel provides an outstanding combination of improved forming and welding characteristics, while providing superior resistance to oxidation, corrosion, ridging and .. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ASTM D638 |
A. Schulman ComAlloy Comshield® 120 Copolymer Polypropylene, Electrically Conductive - Carbon Black Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 32.0 - 40.0 MPa | 4640 - 5800 psi | ASTM D638 |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
Tensile Strength, Ultimate | 32.0 - 40.0 MPa | 4640 - 5800 psi | ASTM D638 |
Arkema Group VOLTALEF® 302 PCTFE VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ASTM D412 |
BASF Elastollan® 1180A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ASTM D638 |
A. Schulman ComAlloy Comshield® 215 High Impact Polystyrene, Electrically Conductive - Carbon Black Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ISO 527-1/-2 |
DSM Arnitel® CM551 TPC-ES Heat Resistant Copolyester |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ISO 527 |
LATI LASTIROL TR G/10-V1 ES 10% Glass Fiber Polystyrene (PS) Structural Foam Resin (UL94 V-1)
(discontinued * Description: Lastirol thermoplastics are polystyrene (PS) products. The Lastirols feature excellent dimensional stability, good flowability, and can be molded without any particular problem. Glass f.. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ASTM D412 |
BASF Elastollan® 690A15N Polyester Type Polyurethane Elastomer This grade is FDA compliant, section 177.2600 and 177.1680, for both wet and dry contact with food. The Elastollan 600 Series of products listed are products that are part of a new series of polyes.. |
|||
Tensile Strength, Ultimate | 32.0 - 82.0 MPa | 4640 - 11900 psi | Average value: 50.0 MPa Grade Count:107 |
Overview of materials for Acrylic, Impact Modified, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Impact Modified, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ASTM D638 |
ExxonMobil Iotek® 8020 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature .. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ASTM D638 |
ExxonMobil Iotek® 8030 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.Excellent abrasion resistance, impact strength, hardness, and tensile strength. Iotek ionomers provide superb low temperature impact strength when .. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ISO 527-2/1A/5 |
Lubrizol ESTALOC® 59003 Ester-Type, Reinforced Engineering Thermoplastic (European Grade) Description: Estaloc® RETP (Reinforced Engineering Thermoplastic) is a tough, dimensionally stable, abrasion-resistant thermoplastic that withstands demanding environments. Developed as an extensio.. |
|||
Tensile Strength, Ultimate | 32.0 MPa | 4640 psi | ASTM D412 |
KKPC KOSYN KTR 602 Thermoplastic Elastomer (TPE) Thermoplastic Elastomer (TPE)Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics .. |