Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.600 J/cm
1.12 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP KONDUIT OX11315 PPS (Asia Pacific)
Thermally conductive electrically insulative mineral filled PPS FR compound.
Izod Impact, Unnotched 0.600 - 7.21 J/cm
1.12 - 13.5 ft-lb/in
Average value: 3.41 J/cm Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Carbon Black Filled". Each property range of values reported is m..
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RE 324 Rigid PVC, Extrusion
Furniture profiles
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RE 412 Rigid PVC, Extrusion
Electric channels
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RE 418 Rigid PVC, Extrusion
Electric channels
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RE 425 Rigid PVC, Extrusion
Electric channels
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RE 425/R Rigid PVC, Extrusion
Shiny electric channels
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RE 625 Rigid PVC, Extrusion
Spiral pipes
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RE 925 Rigid PVC, Extrusion
Various profiles
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RH 306/W Rigid PVC, Antishock Extrusion
Antishock profiles
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RI 059/1 Rigid PVC, Injection Molding
Fittings high fluidity
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RI 50 Rigid PVC, Injection Molding
Technical items
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RK 317/UV Rigid PVC, Extrusion Lead Free
Profiles anti-UV
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RKI 0223 Rigid PVC, Antishock Injection Molding Lead Free
Fittings for building trade
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RKI 0822 Rigid PVC, Antishock Injection Molding Lead Free
Technical items
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RST 0447/1 Rigid PVC, Extrusion Lead Free
Extrusion transparent films
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds R 218 Rigid PVC, Extrusion
Shutters and shiny profiles
Izod Impact, Unnotched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
A. Schulman ComAlloy Comshield® 220 ABS, Electrically Conductive - Carbon Black Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 0.600 J/cm
1.12 ft-lb/in
ASTM D256
A. Schulman ComAlloy Comshield® 215 High Impact Polystyrene, Electrically Conductive - Carbon Black Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RE 220 Rigid PVC, Extrusion
Various profiles
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RE 430 Rigid PVC, Extrusion
Electric channels
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds R 314 Rigid PVC, Extrusion
Electric channels and various profiles
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RE 230/D Rigid PVC, Extrusion
Electric channels
Izod Impact, Unnotched 0.600 - 1.00 J/cm

@Temperature 23.0 °C
1.12 - 1.87 ft-lb/in

@Temperature 73.4 °F
ISO R180
Fainplast Compounds RI 52/S Rigid PVC, Injection Molding
Fittings for building trade