Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648
RheTech Products HP521-00 15% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648
RheTech Products HP521-00UV 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Natural
Applications: Interior trimIP structural componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648
RheTech Products HP521-01 15% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior trimIP structural componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
120°C/h; ISO 75/1
Polykemi AB POLYabs T00 GF20 ABS, Glass Fibre-Reinforced
Information provided by Polykemi AB
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648
PTS PCA-30G00 Impact Modified Polycarbonate/PBT Alloy
For Cold Temperature Impact.Information provided by Polymer Technology and Services, LLC (PTS).
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
SABIC Innovative Plastics LNP LUBRICOMP BX03658N SAN
LNP* LUBRICOMP* BX03658N is a compound based on SAN resin containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerances, good for Water Meter A..
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ISO 75
Polycasa SAN
QUINN SAN sheets are characterized by good optical properties and a brilliant surface. The QUINN SAN range contains sheets that are easy to handle, to vacuum form, and show a very good dimensional s..
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
Unannealed; ASTM D648
Phillips 66 COPYLENE® CH350 Polypropylene Homopolymer
COPYLENE™ CH350 is a controlled rheology, barefoot homopolymer designed for application as a base resin for compounding, consumer products and other injection molding applications.Applications: Inj..
Deflection Temperature at 0.46 MPa (66 psi) 101 °C

@Thickness 6.40 mm
214 °F

@Thickness 0.252 in
Unannealed; ASTM D648
LG Chemical LG703W ABS, Low Gloss, Heat Resistance
Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Filllar Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided..
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ISO 75B
Lucite International Diakon® CLH952 Acrylic Polymer
Information provided by Lucite International
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
Ineos ABS Lustran® Elite HH 1891
Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ISO 75-1/-2
Styrolution Luran® 378 P Crystal Clear Transparent SAN
Description: Easy-flow grade with enhanced resistance to chemicals.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
annealed; ASTM Test
Styrolution Luran® S 757 G ASA
Luran S 757 G is an easy flowing injection molding ASA grade with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ISO 75-1/-2
Styrolution Luran® S 757 G UV White 37019 ASA
Description: Particularly easy flowing injection molding grade for difficult moldings with large flow path/wall thickness ratios.Information provided by STYROLUTION, which is a joint venture between..
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ISO 75-1/-2
Styrolution Luran® S 776 S Colored ASA
Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j..
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ISO 75-1/-2
Styrolution Luran® S 777 K UV Black 56625 ASA
Description: Easy flowing injection molding grade with good toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
annealed; ASTM Test
Styrolution Terluran® GP-35 ABS
Terluran GP-35 is a very high flow grade of ABS for injection molding with good resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF an..
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ISO 75
Styrolution Terluran® SP-6 ABS
Description: High impact grade, suitable for extrusion.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ISO 75-2
Borealis Daplen™ EE340AE Polypropylene TPO Compound
Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q..
Deflection Temperature at 0.46 MPa (66 psi) >= 101 °C
>= 214 °F
ASTM D648
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene
DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible..
Deflection Temperature at 0.46 MPa (66 psi) >= 101 °C
>= 214 °F
ASTM D648
A. Schulman POLYFORT™ PP 2801 Homopolymer Polypropylene
DescriptionPolyfort® PP 2801 is a 12 melt flow homopolymer polypropylene based on the same ingredients as Eastman P4G4Z-001. It is compounded on equipment and under conditions as close as possible..
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
DIN 53461
Polyram RamShine PAS701 ASA, UV Stabilized
UV stabilized general purpose injection molding ASAInformation provided by Polyram Ram On Ind.
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ISO 75
Polyram RamShine PAS702 ASA, UV Stabilized
UV stabilized, general purpose, injection molding ASA.Information provided by Polyram.
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ISO 75-1,-2
Covestro Bayblend® FR3006 HF PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ISO 75-1,-2
Covestro Bayblend® FR3100 TV PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ISO 75-1,-2
Covestro Bayblend® FR3110 TV PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec..
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648
Braskem H 604 Thermoforming & Extrusion Polypropylene Homopolymer
Transparent packaging for food; Flat and corrugated sheets for school and office folders.Information provided by Braskem.
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648
RheTech Products HP501-01 High Performance Polypropylene Copolymer, Non-UV Stabilized, Black
Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 101 - 149 °C
214 - 300 °F
Average value: 129 °C Grade Count:24
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..