Polymer Property : Electrical Resistivity = 1000 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Electrical Resistivity 0.200 - 1000 ohm-cm
0.200 - 1000 ohm-cm
Average value: 257 ohm-cm Grade Count:4
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va..
Electrical Resistivity 0.100 - 1000 ohm-cm
0.100 - 1000 ohm-cm
Average value: 258 ohm-cm Grade Count:27
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu..
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
ASTM D257
PolyOne Edgetek® AS-10CF/000 ABS - 10% Carbon Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Electrical Resistivity 10.0 - 1000 ohm-cm
10.0 - 1000 ohm-cm
ASTM D257
PolyOne Stat-Tech™ PI-10SS/000 Polyetherimide - 10% Stainless Steel Fiber  (discontinued **)
Data provided by PolyOne.
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
ASTM C611
Techmer ES Electrafil® J-1/CF/10 Nylon 66, 10% Carbon Fiber Reinforced
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
ASTM C611
Techmer ES Electrafil® J-50/CF/10/TF/13/SI/2 Polycarbonate, 10% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
ASTM C611
Techmer ES Electrafil® J-50/CF/10/TF/15 Polycarbonate, 10% Carbon Fiber Reinforced, 15% PTFE
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
A. Schulman ComAlloy Comshield® 220 ABS, Electrically Conductive - Carbon Black Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
A. Schulman ComAlloy E-16674B PPS, Electrically Conductive - Carbon Fiber Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
A. Schulman ComAlloy E-16831B Polycarbonate, Electrically Conductive - Carbon Fiber Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Electrical Resistivity 100 - 1000 ohm-cm
100 - 1000 ohm-cm
A. Schulman ComAlloy Comshield® 215 High Impact Polystyrene, Electrically Conductive - Carbon Black Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
Electrical Resistivity 1.00 - 1000 ohm-cm
1.00 - 1000 ohm-cm
ASTM D257
PolyOne Edgetek® AT-000/07SS Copolymer Acetal - 7% Stainless Steel Fiber  (discontinued **)
Data provided by PolyOne.