Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 100 - 1.00e+18 ohm-cm | 100 - 1.00e+18 ohm-cm | Average value: 1.42e+16 ohm-cm Grade Count:81 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Electrical Resistivity | 100 - 1.30e+13 ohm-cm | 100 - 1.30e+13 ohm-cm | Average value: 1.00e+12 ohm-cm Grade Count:5 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Electrical Resistivity | 100 - 1.00e+7 ohm-cm | 100 - 1.00e+7 ohm-cm | Average value: 1.82e+6 ohm-cm Grade Count:11 |
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Carbon Fiber Filled". Each property range of values reported is minimum .. |
|||
Electrical Resistivity | 100 - 1.00e+18 ohm-cm | 100 - 1.00e+18 ohm-cm | Average value: 7.19e+16 ohm-cm Grade Count:13 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Glass Fiber Filler". Specific grades with glass content between 25%.. |
|||
Electrical Resistivity | 100 - 1.00e+6 ohm-cm | 100 - 1.00e+6 ohm-cm | Average value: 117000 ohm-cm Grade Count:15 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |
|||
Electrical Resistivity | 100 - 1.00e+18 ohm-cm | 100 - 1.00e+18 ohm-cm | Average value: 4.11e+16 ohm-cm Grade Count:70 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Electrical Resistivity | 100 - 1000 ohm-cm | 100 - 1000 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-1/CF/10 Nylon 66, 10% Carbon Fiber Reinforced |
|||
Electrical Resistivity | 100 - 1000 ohm-cm | 100 - 1000 ohm-cm | ASTM C611 |
Techmer ES Electrafil® J-50/CF/10/TF/13/SI/2 Polycarbonate, 10% Carbon Fiber Reinforced, 13% PTFE, 2% Silicone |
|||
Electrical Resistivity | 100 ohm-cm - 1e+05 | 100 ohm-cm - 1e+05 | ASTM C611 |
Techmer ES Electrafil® J-50/CF/20/TF/15 Polycarbonate, 20% Carbon Fiber Reinforced, 15% PTFE |
|||
Electrical Resistivity | <= 100 ohm-cm @Temperature 1000 °C |
<= 100 ohm-cm @Temperature 1830 °F |
ASTM D1829 |
CoorsTek TTZ (Dura-Z™) MgO Partially Stabilized Zirconia Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Electrical Resistivity | 100 - 1000 ohm-cm | 100 - 1000 ohm-cm | |
A. Schulman ComAlloy Comshield® 220 ABS, Electrically Conductive - Carbon Black Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Electrical Resistivity | 100 - 1000 ohm-cm | 100 - 1000 ohm-cm | |
A. Schulman ComAlloy E-16674B PPS, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Electrical Resistivity | 100 - 1000 ohm-cm | 100 - 1000 ohm-cm | |
A. Schulman ComAlloy E-16831B Polycarbonate, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Electrical Resistivity | 100 - 1000 ohm-cm | 100 - 1000 ohm-cm | |
A. Schulman ComAlloy Comshield® 215 High Impact Polystyrene, Electrically Conductive - Carbon Black Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Electrical Resistivity | 100 ohm-cm | 100 ohm-cm | ASTM D257 |
PolyOne Edgetek® NI-30CF/000 Nylon 6/10 - 30% Carbon Fiber Reinforced
(discontinued **) Data provided by PolyOne. |
|||
Electrical Resistivity | 100 - 9.90e+9 ohm-cm | 100 - 9.90e+9 ohm-cm | Average value: 6.61e+8 ohm-cm Grade Count:19 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |
|||
Electrical Resistivity | 100 - 1.00e+17 ohm-cm | 100 - 1.00e+17 ohm-cm | Average value: 1.55e+15 ohm-cm Grade Count:122 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Electrical Resistivity | 100 - 1.00e+16 ohm-cm | 100 - 1.00e+16 ohm-cm | Average value: 5.17e+15 ohm-cm Grade Count:6 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |