Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotch-Weld™ DP640 Structural Adhesive

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch-Weld™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch-Weld™ DP640 Structural Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properly abraded and cleaned plastics. Good adhesion can also be obtained on etched aluminum as well as primed aluminum, steel glass. For maximum bond durability under moisture conditions, priming of glass and metal substrates is required.Information provided by 3M
Physical Properties Metric English Comments
Viscosity 25000 cP
25000 cP
Brookfield Viscosity 10000 - 40000 cP
10000 - 40000 cP
Base, RVF #6 sp @ 10 rpm
15000 - 55000 cP
15000 - 55000 cP
Accelerator, RVF #5 sp @ 10 rpm
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 80
70 - 80
ASTM D2240
Elongation at Break 100 %
100 %
ASTM D882
Shear Strength 13.8 MPa
2000 psi
Electrical Properties Metric English Comments
Volume Resistivity 2.60e+12 ohm-cm
2.60e+12 ohm-cm
ASTM D257
Dielectric Constant 5.9

@Frequency 1000 Hz
5.9

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.5 kV/mm
470 kV/in
ASTM D149
Dissipation Factor 0.12

@Frequency 1000 Hz
0.12

@Frequency 1000 Hz
ASTM D150
Processing Properties Metric English Comments
Cure Time 360 - 480 min
6.00 - 8.00 hour
Time to Handling Strength
10100 min
168 hour
Full Cure
Descriptive Properties Value Comments
Appearance Brown
Users viewing this material also viewed the following: