Polymer Property : Brookfield Viscosity = 55000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Brookfield Viscosity 35000 - 55000 cP
35000 - 55000 cP
Acecelerator, DV-II, #7 sp, 20 rpm
3M Scotch-Weld™ DP8005 Black Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Brookfield Viscosity 15000 - 55000 cP
15000 - 55000 cP
Accelerator, RVF #5 sp @ 10 rpm
3M Scotch-Weld™ DP640 Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properl..
Brookfield Viscosity 35000 - 55000 cP
35000 - 55000 cP
Acecelerator, DV-II, #7 sp, 20 rpm
3M Scotch-Weld™ DP8005 Translucent Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8005 is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of polypropyl..
Brookfield Viscosity 10000 - 55000 cP
10000 - 55000 cP
Base, RVF #6 sp @ 20 rpm
3M Scotch-Weld™ 3532 B/A Two-Part Structural Adhesive
3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie..