Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | |
ND Industries 560 Shaft & Bearing Retainer Retaining Compound High Temperature retainer for bushings and sleeves. Retains rotors to shaftsMeets military spec Mil-R-46082B Type II |
|||
Shear Strength | 13.8 MPa | 2000 psi | |
NextGen Adhesives G907-08 Epoxy Adhesive Description: NGAC G907-08 is a low viscosity, electrically insulating, heat cured and 2-part adhesive systems designed for applications where temperature and chemical resistance is critical. The NGA.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | Cured 2 hours at 125°C, Au/Au |
Resin Technology Group TIGA 908 Gold Bonder - Low Stress Silver Conductive 100 parts resin to 6 parts hardener.TIGA 908 is a low stress, conductive silver filled epoxy adhesive. It is recommended for bonding, and sealing electronic applications which require bonding to gol.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Tensile lap, Al to Al |
Master Bond EP42HT-2Med Epoxy Meets USP Class VI Requirements Description: Master Bond Polymer System EP42HT-2Med is a room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring high temperature resistance along wit.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Bond, Al to Al |
Master Bond EP77M-1 Fast Setting, Silver Conductive Epoxy Description: Master Bond Polymer System EP77M-1 is a two component, silver filled, electrically conductive adhesive for high performance bonding and sealing formulated to cure at room temperature or.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Tensile lap, Al to Al |
Master Bond EP42HT-2 Epoxy Adhesive Resists Sterilization Description: Master Bond Polymer System EP42HT-2 is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material featuring high temperature resistance along with o.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Tensile, Al to Al |
Master Bond Supreme 11HT-LO Adhesive and Sealant Serviceable to +400°F Description: Master Bond Polymer System Supreme 11HT-LO is an easy to use two part epoxy adhesive/sealant combining both high shear and high peel strengths along with a relatively fast cure at room .. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 301 Spectrally Transparent Epoxy Product Description: EPO-TEK® 301 is a two component, room temperature curing epoxy featuring very low viscosity, and excellent optical-mechanical properties.Advantages & Application Notes: Semicon.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy Product Description: EPO-TEK® 301-2FL is a two component optical, medical, and semiconductor grade epoxy resin. It is a more flexible version of EPO-TEK® 301-2.Advantages & Application Notes: Sug.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 302-3M Optically Transparent Epoxy Product Description: EPO-TEK® 302-3M is a two component epoxy used for optical, medical, fiber optic, and semiconductor applications. The epoxy is good for adhesive joining, sealing, potting, or as.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 320NC Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy Product Description: EPO-TEK® 377H is a two component, high Tg, graphite filled epoxy designed for ESD/EMI shielding of semiconductor devices and electronics. It can be used in many electronic ind.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® 383ND High Temperature Epoxy Material Description: A slightly longer pot life version of EPO-TEK®353ND designed for high temperature, optical and structural applications inside the semiconductor, hybrid, electronic, fiber opti.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® H35-175MP Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H35-175MP is a single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and opto-elec.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Lap |
Epoxy Technology EPO-TEK® OE120 Two Component Epoxy Material Description: A two component, opaque epoxy, designed for fiber optics packaging applications. It is a black-colored version of EPO-TEK 353ND-T. It has a high Tg for resisting elevated ope.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | Overlap, Al/Al, Hyd Oil 30 days @ RT; ASTM D1002-72 |
3M Scotch-Weld™ 1751 B/A Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 1751 B/A is a gray, aluminum filled, two-part, room temperature curing structural adhesive.Information provided by 3M |
|||
Shear Strength | 13.8 MPa | 2000 psi | Overlap, Steel; ASTM D1002-64 |
3M Scotch-Weld™ CA50 Gel Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. High-viscosity, non-sag gel and less sensitive to acidic surfaces.Information provided by 3M |
|||
Shear Strength | 13.8 MPa | 2000 psi | Overlap, Galvanized Steel Okite degrease Hot dip |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Shear Strength | 13.8 MPa @Temperature 49.0 °C |
2000 psi @Temperature 120 °F |
Overlap, Cohesive Failure |
3M Scotch-Weld™ DP810 Black Structural Adhesive 3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | Lap, Alum to Alum |
Atom Adhesives AA-BOND FDA15 Epoxy Adhesive AA-BOND FDA15 is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Administr.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | cured |
Atom Adhesives AA-DUCT CG2 Epoxy Adhesive AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulati.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | |
Aremco Aremco-Bond™ 2335 Ultra High Temperature Epoxy Ceramic-Filled, Low Expansion, High Lap-Shear Strength & Chemical Resistance, Low Outgassing. |
|||
Shear Strength | 13.8 - 20.7 MPa | 2000 - 3000 psi | Lap; ASTM D1002 |
3M Scotch-Weld™ RT20 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |
|||
Shear Strength | 13.8 MPa | 2000 psi | |
Dymax Magnet Bonder™ 2000 Adhesive DYMAX® Magnet Bonder™ Adhesives for Higher Performance and Lower CostDymax 2000 Magnet Bonder™ AdhesiveFastest cure; bond ferrite to steel. Typical Use: Loudspeaker magnet to pole piece. |
|||
Shear Strength | 13.8 MPa @Temperature -53.0 °C |
2000 psi @Temperature -63.4 °F |
Overlap, Etched Aluminum; ASTM D1002 |
3M Scotch-Weld™ 2216 B/A Tan NS Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel.. |
|||
Shear Strength | >= 13.8 MPa | >= 2000 psi | Tensile, Al to Al |
Master Bond Supreme 10HTFL One Part Epoxy Cures at 250°F Description: Master Bond Polymer System Supreme 10HTFL features a blend of physical properties including outstanding peel strength, very high shear strength and a wide service temperature range of 4.. |