Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 10100 min @Temperature 23.0 °C |
168 hour @Temperature 73.4 °F |
|
Parker Chomerics CHO-BOND 1030 Conductive Silicone Gasket Adhesive Electrically conductive one-component silicone-based RTV adhesive which greatly simplifies the problem of bonding conductive silicone EMI gaskets to metal substrates. This adhesive cures on exposure.. |
|||
Cure Time | 10100 min @Temperature 24.0 °C |
168 hour @Temperature 75.2 °F |
|
Parker Chomerics Tecknit® 0035 Conductive Silicone Sealant/Adhesive Comments: Thin flexible pasteTypical Applications: Bonding elastomer gasketInformation provided by Chomerics |
|||
Cure Time | 10100 min @Temperature 24.0 °C |
168 hour @Temperature 75.2 °F |
|
Parker Chomerics Tecknit® 0192/0193 Conductive Silicone Sealant/Adhesive Comments: Rec. bond line thickness: < 0.4 mm; flexible past.Typical Applications: Bonding Ag/Cu elastomer gaskets; thin bond gap.Information provided by Chomerics |
|||
Cure Time | 10100 min | 168 hour | |
Parker Chomerics Tecknit CON/RTV-Ni 2 Part Nickel Filled RTV Description: TECKNIT electrically conductive, medium viscosity adhesive- sealant system. It is formulated with a special conductive material producing its own unique advantages. After full cure, the.. |
|||
Cure Time | 10100 min | 168 hour | Tack-Free Time |
3M AC-730 Class C-4 (168) Aerospace Sealant 3M Aerospace Sealant AC-730 Class C are two-part, manganese-cured, non-chromate corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corrosion on a.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ EG 515 Urethane Ceramic Rebuild Scotchkote Urethane Ceramic Rebuild EG 515 has been specifically developed as a 100% solids repair system with a degree of flexibility for rebuilding and resurfacing equipment operating in fluid flo.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ FB 857 Urethane Floor Coating Scotchkote Urethane Floor Coating FB 857 has been specifically developed as a 100% solids protection system with a degree of flexibility for application to concrete and asphalt floor surfaces.Produc.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ FG 502 Epoxy Metal Repair Scotchkote Epoxy Metal Repair FG 502 has been specifically developed as a 100% solids epoxy coating for resurfacing and reforming metal machinery and equipment. It also combines good application cha.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ GP 830 WB Epoxy Primer 3M Scotchkote WB Epoxy Primer GP 830 is a member of a range of Scotchkote waterborne coatings and has been specifically developed as a primer/tie coat for use on sealed mineral surfaces and existing.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ PR 415 Epoxy Concrete Repair Scotchkote Epoxy Concrete Repair PR 415 has been specifically developed as a three component 100% solids self priming concrete repair system.Product Features:Combines good application characteristic.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ UV 840 Urethane Coating Scotchkote Urethane Coating UV 840 has been developed to provide a durable gloss finish for use as the final coat of 3M coating systems in the construction and transport industries, where an ease of.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotch-Weld™ LSB90 Flexible Epoxy 3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ 445 Epoxy Slip Deterrent System Scotchkote Epoxy Slip Deterrent System 445 has been specifically developed as a 100% solids system for use with 3M Scotchkote Granular Aggregate to provide a slip deterrent finish to high risk floor.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f.. |
|||
Cure Time | 10100 min @Temperature 23.0 °C |
168 hour @Temperature 73.4 °F |
|
Parker Chomerics CHO-BOND 1038 Conductive Silicone RTV Adhesive Electrically conductive, one component silicone adhesive/sealant that may be used for bonding EMI gaskets or for providing EMI and environmental protection as a caulk. This material cures on exposur.. |
|||
Cure Time | 10100 min @Temperature 23.0 °C |
168 hour @Temperature 73.4 °F |
|
Parker Chomerics CHO-BOND 1075 Silicone RTV Adhesive/Sealant Electrically conductive, one component silicone adhesive/sealant that may be used for bonding EMI gaskets or for providing EMI and environmental protection as a caulk. This material cures on exposur.. |
|||
Cure Time | 10100 min | 168 hour | On-Part Life |
Loctite® 7471 Acetone/Isopropanol Base Primer T Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the .. |