Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 10100 min @Temperature 23.0 °C |
168 hour @Temperature 73.4 °F |
|
Parker Chomerics CHO-BOND 4660 Conductive Caulk/Sealant CHO-BOND® 4660 caulking compound is a single-component, electrically conductive, paste-like material intended for EMI shielding and grounding applications. Its non-hardening characteristic makes it.. |
|||
Cure Time | 10100 min @Temperature 23.0 °C |
168 hour @Temperature 73.4 °F |
|
Parker Chomerics CHO-BOND 4669 Conductive Caulk/Sealant Chomerics two-component conductive epoxy caulks provide excellent adhesion to dissimilar substrates and can be used in lap or butt joint applications. They feature large silver-plated-copper particl.. |
|||
Cure Time | 10100 min @Temperature 24.0 °C |
168 hour @Temperature 75.2 °F |
|
Parker Chomerics CHO-BOND® 1121 General Purpose Adhesive-Sealant Silver Silicone Description: Xylene-free version of CHO-BOND 1038; rec. bond line thickness: > 0.18 mm; primer promotes adhesion CHO-BOND® 1121 is an electrically conductive, one-component silicone adhesive-sealan.. |
|||
Cure Time | 10100 min | 168 hour | @ RT |
Parker Chomerics CHO-SHIELD® 611 Part A Conductive Coating Comments: Variant of CHO-SHIELD 596Typical Applications:Protecting EMI flangesInformation provided by Chomerics |
|||
Cure Time | 10100 - 30200 min @Temperature 24.0 °C |
168 - 504 hour @Temperature 75.2 °F |
|
Parker Chomerics Tecknit® 73-00008 Electrically Conductive Acrylic and Polyurethane Paint Description: TECKNIT manufactures a highly conductive acrylic and polyurethane paints filled with silver. These coatings provide a cost effective method for shielding and grounding plastic enclosure.. |
|||
Cure Time | 10100 min | 168 hour | Tack-Free Time |
3M AC-730 Class C-4 (168) Aerospace Sealant 3M Aerospace Sealant AC-730 Class C are two-part, manganese-cured, non-chromate corrosion inhabiting sealants. These Sealants provide an effective barrier against the common causes of corrosion on a.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ EG 515 Urethane Ceramic Rebuild Scotchkote Urethane Ceramic Rebuild EG 515 has been specifically developed as a 100% solids repair system with a degree of flexibility for rebuilding and resurfacing equipment operating in fluid flo.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ GP 120 Epoxy Primer Scotchkote Epoxy Primer GP 120 has been specifically developed as an anti corrosive coating for steel structures that cannot be abrasive blast cleaned.Product Features:Suitable for use on mechanical.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ HB 850 Epoxy Floor Coating Scotchkote Epoxy Floor Coating HB 850 has been specifically developed as a 100% solids protection system for application to a wide rage of floor surfaces.Product Features:Combines good application c.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ MC 145 Epoxy Primer Scotchkote Epoxy Primer MC 145 is a solvent based two component primer suitable for use on a wide range of metallic and glass reinforced plastic (GRP) surfaces prior to the application of Scotchkote.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ RS 820 Epoxy Screed Scotchkote Epoxy Sceed RS 820 has been specially developed as a three component 100% solids resurfacing screed for application to concrete floor surfacesProduct Features:Combines good application ch.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ XF 895 Fast Curing Floor Coating Scotchkote Fast Curing Floor Coating XF 895 has been specifically developed as a high build floor protection system for application to concrete surfaces, to provide rapid return to serviceProduct Fe.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ 165HB Urethane Coating 3M Scotchkote Urethane Coating 165HB is a two component 100% solids urethane coating used for the internal and external protection of steel and concrete pipes, tanks, and vessels. It can be used in .. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotchkote™ SP 810 Epoxy Sealer Scotchkote Epoxy Sealer SP 810 has been specifically developed as a low viscosity primer/sealer for concrete and cementitious surfaces prior to application of other Scotchkote 100% solids epoxy syst.. |
|||
Cure Time | 10100 min @Temperature 23.0 °C |
168 hour @Temperature 73.4 °F |
|
Parker Chomerics CHO-BOND 1038 Conductive Silicone RTV Adhesive Electrically conductive, one component silicone adhesive/sealant that may be used for bonding EMI gaskets or for providing EMI and environmental protection as a caulk. This material cures on exposur.. |
|||
Cure Time | 10100 min @Temperature 24.0 °C |
168 hour @Temperature 75.2 °F |
|
Parker Chomerics CHO-SHIELD® 2002 Conductive Coating Electrically conductive coatings provide corrosion protection for enclosure flanges which mate with EMI shielding gaskets. They can also provide a corrosion resistant conductive surface coating on a.. |
|||
Cure Time | 10100 min | 168 hour | Full Cure |
3M Scotch-Weld™ 3549 B/A Two-Part Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-component, polyurethane adhesives which cure at room temperature or with heat to form tough, impact-resistant structural bonds. Their adhesion propertie.. |
|||
Cure Time | 10100 min | 168 hour | On-Part Life |
Loctite® 7471 Acetone/Isopropanol Base Primer T Surface PreparersLoctite offers a complete line of surface preparation products to ensure the maximum performance of Loctite® Adhesives and Sealants.Loctite® Accelerators are used to increase the .. |