Electrical Properties Metric English Comments
Dielectric Strength 18.5 kV/mm
470 kV/in
ASTM D149
Proto3000 Duraform® EX Selective Laser Sintering (SLS®) Prototyping Polymer
Plastic for use with all Sinterstation® Pro and Sinterstation HiQ™ series SLS® systemsDescription: This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and..
Dielectric Strength 18.5 - 100 kV/mm
470 - 2540 kV/in
Average value: 26.3 kV/mm Grade Count:49
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Dielectric Strength 18.5 - 45.0 kV/mm
470 - 1140 kV/in
Average value: 27.7 kV/mm Grade Count:23
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Dielectric Strength 18.5 kV/mm
470 kV/in
Momentive Performance Materials RTV577 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White
RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DBT (dibutyl tin dilaurate) as the stand..
Dielectric Strength 18.5 kV/mm

@Thickness 1.91 mm
470 kV/in

@Thickness 0.0750 in
Momentive Performance Materials RTV577 White Extreme Low Temperature Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Dielectric Strength 18.5 kV/mm

@Thickness 1.91 mm
470 kV/in

@Thickness 0.0750 in
Momentive Performance Materials RTV8262 Red General Purpose Potting/Encapsulating Compound
Two-part condensation cure. Two-part condensation cure silicones RTVs are designed to cute at room temperature, and can be applied at temperature up to one inch (2.5 cm). These are very tough mate..
Dielectric Strength 18.5 kV/mm
470 kV/in
Momentive Performance Materials RTV8262 Silicone Rubber Compounds for Potting, Encapsulating and Sealing
RTV8111, RTV8112 and RTV8262 silicone rubber compounds are two-part silicone elastomers supplied in ready-to-use matched kits containing a base compound and curing agent.Mechanical and electrical pr..
Dielectric Strength 18.5 kV/mm
470 kV/in
Perpendicular (ASTM D149), in Oil
Haysite HCR-197 Corrosion Resistant Polyester/Glass Sheet
A fiber glass reinforced thermoset polyester sheet using ATLAC® 382 Bisphenol-A Fumarate in the resin matrix. Standard color is light yellow. Additional data covering resistance to specific chemi..
Dielectric Strength 18.5 kV/mm
470 kV/in
Method A (Short-Time); ASTM D149
Techmer ES Plastiblend® PA6/6,6 GF50 HS L 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, Copolymer and Lubricat..
Dielectric Strength 18.5 kV/mm

@Thickness 3.20 mm
470 kV/in

@Thickness 0.126 in
in oil; IEC 60243-1
SABIC Innovative Plastics NORYL GTX GTX924 PPE+PA (Europe-Africa-Middle East)
NORYL GTX 924 is an UV stabilized unfilled Noryl GTX grade with improved processability. Noryl GTX 924 is specially designed for wheeltrim applications.
Dielectric Strength 18.5 kV/mm

@Thickness 1.02 mm
470 kV/in

@Thickness 0.0400 in
60 cycles AC avg. RMS; ASTM-D149
CoorsTek ADSR-96R DuraStrate™ 96% Alumina Thick Film
Applications: thick films and lasers
Dielectric Strength 18.5 kV/mm
470 kV/in
Dow Corning 3-4130 DIELECTRIC GEL KIT
Two-part, clear, heat cure, low extractables.Information provided by Dow Corning
Dielectric Strength 18.5 kV/mm
470 kV/in
ASTM D149
3D Systems DuraForm® EX Impact-Resistant Plastic for SLS® Systems
This impact-resistant plastic offers the toughness of injection-molded polypropylene and ABS and is suitable for Rapid Manufacturing. For use with all Sinterstation® Pro and Sinterstation HiQ™ ser..
Dielectric Strength 18.5 kV/mm
470 kV/in
ASTM D149
ALM PA 850-Nat Nylon 11 SLS Prototyping Polymer
Unfilled PA 11 formulated for easy processing. Can be run as a drop-in replacement for other commercially available PA 11 laser sintering powders. Parts produced from PA 850 exhibit outstanding mech..
Dielectric Strength 18.5 kV/mm
470 kV/in
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M
Dielectric Strength 18.5 kV/mm
470 kV/in
ASTM D149
3M 7951 Hi-Performance Acrylic 300MP
This adhesive is designed for applications requiring greater initial adhesion especially to low surface energy (LSE) plastic substrates. Temperature performance is up to 300°F (149°C) for most app..
Dielectric Strength 18.5 kV/mm
470 kV/in
ASTM D149
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..
Dielectric Strength 18.5 kV/mm
470 kV/in
ASTM D149
3M Scotch-Weld™ DP640 Structural Adhesive