Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 360 min | 6.00 hour | Ambient Set |
Reltek BONDiT™ B-481 Adhesive, Sealant & Coating System Key Properties: High strength and toughness with excellent thermal stability to 400°F.Outstanding chemical resistance.Excellent electrical, and mechanical properties.Ease of use.Applications: Encap.. |
|||
Cure Time | 360 min @Temperature 25.0 °C |
6.00 hour @Temperature 77.0 °F |
50% relative humidity |
Lord Adhesives Aeroglaze® K3425 Sandable Primer/Surfacer For application on epoxy graphite or other plastic substrates or over a suitable primer on metal.Limitations - Aeroglaze® K3425 primer/surfacer contains no inhibiting pigments and is not suitable.. |
|||
Cure Time | 360 min | 6.00 hour | To depth of 3.2 mm |
Momentive Performance Materials RTV5242 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Cure Time | 360 min | 6.00 hour | To depth of 3.2 mm |
Momentive Performance Materials RTV5243 Neutral Cure, One Component RTV Adhesive Sealant RTV5240 series sealants are alkoxy neutral cure, one-component, ready to use, electronic grade silicone adhesive sealants exhibiting high strength that will maintain a strong bond even when exposed .. |
|||
Cure Time | 360 min | 6.00 hour | 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3101 Encapsulating Adhesive System TRA-CAST 3101 is an easy-to-use, room temperature cure, rigid, low viscosity, 100% solids (no solvents) epoxy resin and hardener system with excellent mechanical and electrical properties. It is rec.. |
|||
Cure Time | 360 min | 6.00 hour | 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3110 Low Density Epoxy Casting System TRA-CAST 3110 is a unicellular, low density, syntactic-foam epoxy resin casting system of medium viscosity that easily handles, mixes and cures at room temperature. Developed for industrial encapsul.. |
|||
Cure Time | 360 min | 6.00 hour | 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3156 General Purpose Epoxy Casting System TRA-CAST 3156 is an easy-to-use, low cost, versatile epoxy resin and hardener system developed for general purpose casting applications. It develops excellent adhesion to most metals, plastics, and .. |
|||
Cure Time | 360 min | 6.00 hour | 2 hrs @ 65°C + 4 hrs @ 130°C |
Tra-Con Tra-Cast 3357 High Temperature Rigid Epoxy Casting System TRA-CAST 3357 is a smooth pouring, low viscosity casting resin system recommended for rigid, large mass potting, encapsulating, laminating, filament-winding and coil embedment applications where the.. |
|||
Cure Time | 360 min | 6.00 hour | 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3107 Low Shrinkage Epoxy Casting System TRA-CAST 3107 is a versatile epoxy casting system developed for high performance production potting, encapsulating, casting and tooling applications where low shrinkage, easy handling and flowabilit.. |
|||
Cure Time | 360 min | 6.00 hour | 4 hrs @ 25°C + 2 hrs @ 65°C |
Tra-Con Tra-Cast 3143 Fire Retardant Epoxy Casting Compound TRA-CAST 3143 has a low viscosity and long pot life. It is certified to the requirements of UL 94 V-O, and is recommended for rigid potting, laminating, transformer encapsulating, filament winding a.. |
|||
Cure Time | 360 - 2880 min | 6.00 - 48.0 hour | Full Cure; Unprimed |
Loctite® Gasket Eliminator® 509 Flange Sealant Anaerobic GasketingLoctite® 509 Flexible Cure Gasket Eliminator® Flange SealantProduct withstands minor flange movements caused by vibrations. It will not run when applied to vertical surfaces. F.. |
|||
Cure Time | 360 - 420 min | 6.00 - 7.00 hour | Tack-Free Time |
3M AC-350 Class C-2 Aerospace Sealant 3M Aerospace Sealant AC-350 Class C are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant hav.. |
|||
Cure Time | 360 - 480 min | 6.00 - 8.00 hour | Tack Free Time, catalyzed with QM cat BLUE |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Cure Time | 360 min | 6.00 hour | Touch Dry |
3M Scotchkote™ 162HB Epoxy Coating 3M Scotchkote Epoxy Coating 163HB has been specifically developed as a 100% solids lining for the internals of pipes, tanks, vessels and other equipment in contact with fresh water, sea water, raw w.. |
|||
Cure Time | 360 min | 6.00 hour | Touch Dry |
3M Scotchkote™ GP 120 Epoxy Primer Scotchkote Epoxy Primer GP 120 has been specifically developed as an anti corrosive coating for steel structures that cannot be abrasive blast cleaned.Product Features:Suitable for use on mechanical.. |
|||
Cure Time | 360 min @Temperature 24.0 °C |
6.00 hour @Temperature 75.2 °F |
demold time |
BCC Products METAL-KAST/SLO BC 8010-2 Urethane Casting BC8010-2 Metal-Kast/Slo, the result of extensive research and development is an aluminum filled, metal-like, medium setting urethane reproduction plastic. A slower version of the BC8010 Metal-Kast w.. |
|||
Cure Time | 360 min | 6.00 hour | Full Cure |
3M Scotch-Weld™ DP604NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesive DP-604NS is a black, rapid setting, two-component polyurethane. It is packaged as 1:1 ratio liquids in a duo-pak cartridge. With the squeeze of the trigger, the .. |
|||
Cure Time | 360 - 420 min | 6.00 - 7.00 hour | Tack-Free Time |
3M AC-370 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solven.. |
|||
Cure Time | 360 - 420 min | 6.00 - 7.00 hour | |
3M AC-370 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-370 Class B are fast cure, low density polysulfide sealants suitable for fuel tank and fuselage applications. These two-component, manganese dioxide cured sealants are solven.. |
|||
Cure Time | 360 min @Temperature 121 °C |
6.00 hour @Temperature 250 °F |
Alternate Cure |
Aremco Aremco-Bond™ 2315 High Performance Epoxide High Temperature, Low Viscosity, Potting Compound for Electrical Applications. |
|||
Cure Time | 360 min | 6.00 hour | |
3M AC-730 Class B-1/2 Aerospace Sealant 3M Aerospace Sealant AC-730 Class B are fast cure, two-part, manganese-cured, non-chromate containing corrosion inhabiting sealants. These Sealants provide an effective barrier against the common ca.. |
|||
Cure Time | 360 min | 6.00 hour | Time to Handling Strength |
3M Scotch-Weld™ DP190 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Translucent is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Translucent but faster curing.Information provided by 3M |
|||
Cure Time | 360 - 480 min | 6.00 - 8.00 hour | Tack Free Time, catalyzed with QM cat BLUE |
ACC QM 113 QSI Quantum Silicones 13 Durometer Condensation Cured Moldmaking Material QM 113 is a two component, room temperature condensation cure silicone material. The cured rubber is very soft, has excellent mechanical properties and good shelf-life stability. This material is an.. |
|||
Cure Time | 360 - 2880 min | 6.00 - 48.0 hour | Full Cure; Unprimed |
Loctite® 573 Semi-rigid Cure Anaerobic Sealant Anaerobic GasketingLoctite® 573 Semi-rigid Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Slow curing for extended assembly operations |