Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® BF-0930 MABS, Unreinforced Scratch Resistant

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® BF-0930 MABS, Unreinforced Scratch Resistant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scratch resistantInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Melt Flow 33 g/10 min

@Load 10.0 kg,
Temperature 220 °C
33 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 56.9 MPa
8250 psi
5 mm/min; ASTM D638
Flexural Strength 87.3 MPa
12700 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 2.16 J/cm

@Thickness 3.17 mm
4.04 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 94.0 °C
201 °F
B/50; ISO R306
Flammability, UL94 HB

@Thickness 1.50 - 3.00 mm
HB

@Thickness 0.0591 - 0.118 in
Descriptive Properties Value Comments
Pencil Hardness 2H
500g, JIS K 5401
Users viewing this material also viewed the following: