Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® GC-0770 H ABS/PET, Unreinforced Recycled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Eco-friendly Post-Consumer recycled PET.Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength at Break 26.5 MPa
3840 psi
50 mm/min; ASTM D638
Tensile Strength, Yield 41.2 MPa
5970 psi
50 mm/min; ASTM D638
Elongation at Break 17 %
17 %
50 mm/min; ASTM D638
Tensile Modulus 1.77 GPa
256 ksi
50 mm/min; ASTM D638
Flexural Strength 49.0 MPa
7110 psi
2.8 mm/min; ASTM D790
Flexural Modulus 1.72 GPa
249 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 1.96 J/cm

@Thickness 6.35 mm
3.67 ft-lb/in

@Thickness 0.250 in
ASTM D256
4.41 J/cm

@Thickness 3.17 mm
8.27 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C

@Thickness 6.40 mm
203 °F

@Thickness 0.252 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 83.0 °C

@Thickness 6.40 mm
181 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 90.0 °C
194 °F
B/50; ISO R306
94.0 °C
201 °F
B/120; ISO R306