Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Infino® HI-1001B PC/ABS, Unreinforced

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® HI-1001B PC/ABS, Unreinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Melt Flow 20 g/10 min

@Load 10.0 kg,
Temperature 250 °C
20 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength, Yield 60.8 MPa
8820 psi
5 mm/min; ASTM D638
Flexural Strength 83.4 MPa
12100 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.45 GPa
356 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 4.41 J/cm

@Thickness 3.17 mm
8.27 ft-lb/in

@Thickness 0.125 in
ASTM D256
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved