Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® VE-0860 ABS, Unreinforced FR

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® VE-0860 ABS, Unreinforced FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flame-retardant ABS with high heat resistance that can be used in battery cases and adaptorsInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm

@Thickness 3.20 mm
0.0030 - 0.0060 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 1.6 g/10 min

@Load 5.00 kg,
Temperature 200 °C
1.6 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Yield 43.1 MPa
6260 psi
5 mm/min; ASTM D638
Flexural Strength 63.7 MPa
9240 psi
2.8 mm/min; ASTM D638
Flexural Modulus 2.26 GPa
327 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 1.37 J/cm

@Thickness 6.35 mm
2.57 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C

@Thickness 6.40 mm
185 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 97.0 °C
207 °F
B/50; ISO R306
Flammability, UL94 V-0

@Thickness 1.50 - 2.70 mm
V-0

@Thickness 0.0591 - 0.106 in
5VB

@Thickness 2.50 - 2.70 mm
5VB

@Thickness 0.0984 - 0.106 in