Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Extruded
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® SP-0183 ABS, Unreinforced Extrusion Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Melt Flow 3.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
3.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 41.2 MPa
5970 psi
5 mm/min; ASTM D638
Elongation at Break 50 %
50 %
5 mm/min; ASTM D638
Flexural Strength 60.8 MPa
8820 psi
2.8 mm/min; ASTM D790
Flexural Modulus 1.86 GPa
270 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 4.02 J/cm

@Thickness 6.35 mm
7.53 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C

@Thickness 6.40 mm
196 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 101 °C
214 °F
B/50; ISO R306
Users viewing this material also viewed the following: