Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 10% Glass Fiber Filled
Manufacturer Samsung, Cheil Industries
Trade Name Starex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Starex® VG-4920 ABS, Glass Filled FR.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm

@Thickness 3.20 mm
0.0010 - 0.0030 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 25 g/10 min

@Load 10.0 kg,
Temperature 220 °C
25 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 88.3 MPa
12800 psi
5 mm/min; ASTM D638
Flexural Strength 103 MPa
14900 psi
2.8 mm/min; ASTM D638
Flexural Modulus 5.88 GPa
853 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 0.490 J/cm

@Thickness 3.17 mm
0.918 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C

@Thickness 6.40 mm
205 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 V-0

@Thickness 1.60 - 3.00 mm
V-0

@Thickness 0.0630 - 0.118 in
5VB

@Thickness 2.00 - 3.00 mm
5VB

@Thickness 0.0787 - 0.118 in