Samsung Cheil Industries Infino® ASF-9810F PBT/PET, Mineral Filled General Purpose

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , PBT + PET, Mineral Filled , Polyethylene Terephthalate (PET)
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® ASF-9810F PBT/PET, Mineral Filled General Purpose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material for automobile lamp with high flowInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Melt Flow 55 g/10 min

@Load 2.16 kg,
Temperature 250 °C
55 g/10 min

@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 60.8 MPa
8820 psi
50 mm/min; ASTM D638
Flexural Strength 83.4 MPa
12100 psi
2.8 mm/min; ASTM D790
Flexural Modulus 2.45 GPa
356 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.294 J/cm

@Thickness 3.17 mm
0.551 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 180 °C
356 °F
B/50; ISO R306
Optical Properties Metric English Comments
Gloss >= 92 %

@Temperature 23.0 °C
>= 92 %

@Temperature 73.4 °F
50% RH, 60°; ASTM D2457
Users viewing this material also viewed the following: