Samsung Cheil Industries Infino® XP-2150IM PPS, 50% Glass Reinforced

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS) , Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
Manufacturer Samsung, Cheil Industries
Trade Name Infino®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Samsung Cheil Industries Infino® XP-2150IM PPS, 50% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPS/GS that is used in mobile phone LCD bracketInformation provided by Samsung Cheil Industries.
Physical Properties Metric English Comments
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Water Absorption 0.020 %

@Temperature 23.0 °C
0.020 %

@Temperature 73.4 °F
ASTM D570
Linear Mold Shrinkage, Flow 0.0025 - 0.010 cm/cm

@Thickness 3.20 mm
0.0025 - 0.010 in/in

@Thickness 0.126 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Yield 157 MPa
22800 psi
5 mm/min; ASTM D638
Elongation at Break 2.2 %
2.2 %
5 mm/min; ASTM D638
Flexural Strength 245 MPa
35500 psi
2.8 mm/min; ASTM D638
Flexural Modulus 14.7 GPa
2130 ksi
2.8 mm/min; ASTM D638
Izod Impact, Notched 0.883 J/cm

@Thickness 3.17 mm
1.65 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 270 °C

@Thickness 6.40 mm
518 °F

@Thickness 0.252 in
ASTM D648
Flammability, UL94 V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm

@Temperature 23.0 °C
1.00e+16 ohm-cm

@Temperature 73.4 °F
50% RH; ASTM D257
Dielectric Constant 5.0

@Frequency 1.00e+6 Hz
5.0

@Frequency 1.00e+6 Hz
ASTM D150
Dissipation Factor 0.0050

@Frequency 1.00e+6 Hz
0.0050

@Frequency 1.00e+6 Hz
ASTM D150