Overview of materials for Polycarbonate, UV Stabilized

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, UV Stabilized
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polycarbonate, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, UV Stabilized". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.15 - 1.55 g/cc
0.0415 - 0.0560 lb/in³
Average value: 1.21 g/cc Grade Count:119
Water Absorption 0.0230 - 0.350 %
0.0230 - 0.350 %
Average value: 0.212 % Grade Count:76
Moisture Absorption at Equilibrium 0.120 - 0.350 %
0.120 - 0.350 %
Average value: 0.149 % Grade Count:29
0.580 - 0.580 %

@Temperature 100 - 100 °C
0.580 - 0.580 %

@Temperature 212 - 212 °F
Average value: 0.580 % Grade Count:1
Water Absorption at Saturation 0.300 - 0.400 %
0.300 - 0.400 %
Average value: 0.314 % Grade Count:25
Water Vapor Transmission 15.0 g/m²/day
0.966 g/100 in²/day
Average value: 15.0 g/m²/day Grade Count:11
Oxygen Transmission 65.0 - 80.0 cc-mm/m²-24hr-atm
165 - 203 cc-mil/100 in²-24hr-atm
Average value: 70.0 cc-mm/m²-24hr-atm Grade Count:12
Nitrogen Transmission 12.0 - 16.0 cc-mm/m²-24hr-atm
30.5 - 40.6 cc-mil/100 in²-24hr-atm
Average value: 13.1 cc-mm/m²-24hr-atm Grade Count:12
Carbon Dioxide Transmission 380 - 480 cc-mm/m²-24hr-atm
965 - 1220 cc-mil/100 in²-24hr-atm
Average value: 417 cc-mm/m²-24hr-atm Grade Count:12
Linear Mold Shrinkage 0.000500 - 0.0100 cm/cm
0.000500 - 0.0100 in/in
Average value: 0.00502 cm/cm Grade Count:90
Linear Mold Shrinkage, Transverse 0.00500 - 0.0100 cm/cm
0.00500 - 0.0100 in/in
Average value: 0.00727 cm/cm Grade Count:22
Melt Flow 3.00 - 46.0 g/10 min
3.00 - 46.0 g/10 min
Average value: 14.0 g/10 min Grade Count:102
Mechanical Properties Metric English Comments
Hardness, Rockwell M 65.0 - 85.0
65.0 - 85.0
Average value: 72.7 Grade Count:31
Hardness, Rockwell R 80.0 - 127
80.0 - 127
Average value: 119 Grade Count:56
Ball Indentation Hardness 100 - 116 MPa
14500 - 16800 psi
Average value: 112 MPa Grade Count:21
Tensile Strength, Ultimate 55.2 - 80.0 MPa
8000 - 11600 psi
Average value: 66.9 MPa Grade Count:79
Tensile Strength, Yield 49.6 - 75.0 MPa
7200 - 10900 psi
Average value: 62.8 MPa Grade Count:97
Elongation at Break 8.00 - 150 %
8.00 - 150 %
Average value: 100 % Grade Count:115
Elongation at Yield 5.00 - 88.0 %
5.00 - 88.0 %
Average value: 7.50 % Grade Count:56
Modulus of Elasticity 2.00 - 2.60 GPa
290 - 377 ksi
Average value: 2.35 GPa Grade Count:63
Flexural Yield Strength 68.0 - 110 MPa
9860 - 16000 psi
Average value: 89.4 MPa Grade Count:101
Flexural Modulus 0.228 - 3.96 GPa
33.0 - 575 ksi
Average value: 2.29 GPa Grade Count:106
Compressive Yield Strength 76.0 - 77.0 MPa
11000 - 11200 psi
Average value: 76.3 MPa Grade Count:3
Izod Impact, Notched 0.500 - 9.77 J/cm
0.937 - 18.3 ft-lb/in
Average value: 7.04 J/cm Grade Count:82
1.00 - 1.80 J/cm

@Temperature -30.0 - -30.0 °C
1.87 - 3.37 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 1.40 J/cm Grade Count:1
1.00 - 1.80 J/cm

@Thickness 3.20 - 3.20 mm
1.87 - 3.37 ft-lb/in

@Thickness 0.126 - 0.126 in
Average value: 1.40 J/cm Grade Count:1
Izod Impact, Unnotched 0.981 J/cm - NB
1.84 ft-lb/in - NB
Average value: 13.3 J/cm Grade Count:26
NB - NB

@Temperature -40.0 - -40.0 °C
NB - NB

@Temperature -40.0 - -40.0 °F
Grade Count:1
Izod Impact, Notched (ISO) 12.0 - 92.0 kJ/m²
5.71 - 43.8 ft-lb/in²
Average value: 73.6 kJ/m² Grade Count:27
25.0 - 25.0 kJ/m²

@Temperature -30.0 - -30.0 °C
11.9 - 11.9 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 13.4 kJ/m² Grade Count:2
12.0 - 16.0 kJ/m²

@Temperature -30.0 - -30.0 °C
5.71 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 13.4 kJ/m² Grade Count:17
12.0 - 16.0 kJ/m²

@Thickness 3.20 - 3.20 mm
5.71 - 7.61 ft-lb/in²

@Thickness 0.126 - 0.126 in
Average value: 13.4 kJ/m² Grade Count:17
Izod Impact, Unnotched (ISO) NB - NB

@Temperature -30.0 - -30.0 °C
NB - NB

@Temperature -22.0 - -22.0 °F
Grade Count:2
Charpy Impact Unnotched 1000 J/cm² - NB
4760 ft-lb/in² - NB
Grade Count:28
999.9 - 999.9 J/cm²

@Temperature -60.0 - -30.0 °C
4759 - 4759 ft-lb/in²

@Temperature -76.0 - -22.0 °F
Grade Count:20
Charpy Impact, Notched 1.20 - 75.0 J/cm²
5.71 - 357 ft-lb/in²
Average value: 9.67 J/cm² Grade Count:22
1.40 - 1.60 J/cm²

@Temperature -30.0 - -30.0 °C
6.66 - 7.61 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.44 J/cm² Grade Count:16
1.40 - 1.60 J/cm²

@Thickness 3.00 - 3.00 mm
6.66 - 7.61 ft-lb/in²

@Thickness 0.118 - 0.118 in
Average value: 1.44 J/cm² Grade Count:16
Dart Drop, Total Energy 72.0 - 169 J
53.1 - 125 ft-lb
Average value: 90.1 J Grade Count:19
Puncture Energy 50.0 - 60.0 J
36.9 - 44.3 ft-lb
Average value: 58.1 J Grade Count:16
55.0 - 70.0 J

@Temperature -30.0 - -30.0 °C
40.6 - 51.6 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 64.7 J Grade Count:16
Tensile Creep Modulus, 1 hour 2200 MPa
319000 psi
Average value: 2200 MPa Grade Count:18
Tensile Creep Modulus, 1000 hours 1900 MPa
276000 psi
Average value: 1900 MPa Grade Count:18
Thermal Properties Metric English Comments
CTE, linear 32.4 - 117 µm/m-°C
18.0 - 65.0 µin/in-°F
Average value: 70.3 µm/m-°C Grade Count:71
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 - 1.00e+18 ohm-cm
1.00e+14 - 1.00e+18 ohm-cm
Average value: 1.11e+17 ohm-cm Grade Count:70
Surface Resistance 1.00e+14 - 1.00e+17 ohm
1.00e+14 - 1.00e+17 ohm
Average value: 1.50e+16 ohm Grade Count:34
Dielectric Constant 2.85 - 3.17
2.85 - 3.17
Average value: 2.99 Grade Count:61
Dielectric Strength 14.9 - 35.0 kV/mm
378 - 889 kV/in
Average value: 24.6 kV/mm Grade Count:69
Dissipation Factor 0.000400 - 0.0110
0.000400 - 0.0110
Average value: 0.00488 Grade Count:61
Arc Resistance 0.000 - 180 sec
0.000 - 180 sec
Average value: 119 sec Grade Count:41
Comparative Tracking Index 100 - 600 V
100 - 600 V
Average value: 234 V Grade Count:54
Hot Wire Ignition, HWI 15.0 - 60.0 sec
15.0 - 60.0 sec
Average value: 41.1 sec Grade Count:25
High Amp Arc Ignition, HAI 15.0 - 120 arcs
15.0 - 120 arcs
Average value: 114 arcs Grade Count:25
High Voltage Arc-Tracking Rate, HVTR 10.0 - 150 mm/min
0.394 - 5.91 in/min
Average value: 65.3 mm/min Grade Count:25